A maximum strain criterion for electric-field-induced fatigue crack propagation in ferroelectric ceramics

被引:26
作者
Shang, JK [1 ]
Tan, XL [1 ]
机构
[1] Univ Illinois, Dept Mat Sci & Engn, Urbana, IL 61801 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2001年 / 301卷 / 02期
关键词
electric field; crack growth; piezoelectric; ferroelectric ceramics;
D O I
10.1016/S0921-5093(00)01812-8
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Crack growth behavior in ferroelectric ceramics was examined under purely electrical and purely mechanical loading conditions. While cracks grew under mechanical loading along the plane of the maximum tensile stress, crack growth under electrical loading tended to be intergranular and the direction of the crack growth was found to vary greatly with geometric arrangements of applied electric field, remnant polarization and crack orientation. When both the applied field and remnant polarization were perpendicular to the crack plane, the crack propagated straight ahead on the original plane. However, for other electrical configurations, cracks were driven to propagate on the planes inclined up to 90 degrees from the original crack plane. Analysis of the electromechanical conditions in the specimens indicated that the crack preferred to propagate on the plane of the maximum principal strain, thus satisfying a maximum strain criterion. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:131 / 139
页数:9
相关论文
共 40 条
[31]  
SMITH TE, 1967, J APPL MECH, P431
[32]   PLANE PROBLEMS IN PIEZOELECTRIC MEDIA WITH DEFECTS [J].
SOSA, H .
INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1991, 28 (04) :491-505
[33]   FRACTURE-MECHANICS FOR PIEZOELECTRIC CERAMICS [J].
SUO, Z ;
KUO, CM ;
BARNETT, DM ;
WILLIS, JR .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1992, 40 (04) :739-765
[34]   MODELS FOR BREAKDOWN-RESISTANT DIELECTRIC AND FERROELECTRIC CERAMICS [J].
SUO, Z .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1993, 41 (07) :1155-1176
[35]   Influence of temperature on the electromechanical and fatigue behavior of piezoelectric ceramics [J].
Wang, D ;
Fotinich, Y ;
Carman, GP .
JOURNAL OF APPLIED PHYSICS, 1998, 83 (10) :5342-5350
[36]   Crack propagation in piezoelectric ceramics: Effects of applied electric fields [J].
Wang, HY ;
Singh, RN .
JOURNAL OF APPLIED PHYSICS, 1997, 81 (11) :7471-7479
[37]   FRACTURE-BEHAVIOR OF CYCLICALLY LOADED PZT [J].
WHITE, GS ;
RAYNES, AS ;
VAUDIN, MD ;
FREIMAN, SW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (10) :2603-2608
[38]   In situ transmission electron microscopy study of electric-field-induced microcracking in single crystal Pb(Mg1/3Nb2/3)O3-PbTiO3 [J].
Xu, Z ;
Tan, X ;
Han, P ;
Shang, JK .
APPLIED PHYSICS LETTERS, 2000, 76 (25) :3732-3734
[39]   CRACKING IN CERAMIC ACTUATORS CAUSED BY ELECTROSTRICTION [J].
YANG, W ;
SUO, Z .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1994, 42 (04) :649-663
[40]  
Zhu T, 1999, J MECH PHYS SOLIDS, V47, P81