Fracture strength of ultrananocrystalline diamond thin films - identification of Weibull parameters

被引:86
作者
Espinosa, HD [3 ]
Peng, B
Prorok, BC
Moldovan, N
Auciello, O
Carlisle, JA
Gruen, DM
Mancini, DC
机构
[1] Argonne Natl Lab, Div Mat Sci, Argonne, IL 60439 USA
[2] Argonne Natl Lab, Expt Facil Div, Argonne, IL 60439 USA
[3] Northwestern Univ, Dept Mech Engn, Evanston, IL 60208 USA
关键词
D O I
10.1063/1.1613372
中图分类号
O59 [应用物理学];
学科分类号
摘要
The fracture strength of ultrananocrystalline diamond (UNCD) has been investigated using tensile testing of freestanding submicron films. Specifically, the fracture strength of UNCD membranes, grown by microwave plasma chemical vapor deposition (MPCVD), was measured using the membrane deflection experiment developed by Espinosa and co-workers. The data show that fracture strength follows a Weibull distribution. Furthermore, we show that the Weibull parameters are highly dependent on the seeding process used in the growth of the films. When seeding was performed with microsized diamond particles, using mechanical polishing, the stress resulting in a probability of failure of 63% was found to be 1.74 GPa, and the Weibull modulus was 5.74. By contrast, when seeding was performed with nanosized diamond particles, using ultrasonic agitation, the stress resulting in a probability of failure of 63%, increased to 4.13 GPa, and the Weibull modulus was 10.76. The tests also provided the elastic modulus of UNCD, which was found to vary from 940 to 970 GPa for both micro- and nanoseeding. The investigation highlights the role of microfabrication defects on material properties and reliability, as a function of seeding technique, when identical MPCVD chemistry is employed. The parameters identified in this study are expected to aid the designer of microelectromechanical systems devices employing UNCD films. (C) 2003 American Institute of Physics.
引用
收藏
页码:6076 / 6084
页数:9
相关论文
共 30 条
[1]  
[Anonymous], P MEMS MECH MEAS S
[2]  
Auciello O, 2000, MATER RES SOC SYMP P, V605, P73
[3]  
Bagdahn J, 2002, MATER RES SOC SYMP P, V687, P285
[4]   Synthesis and characterization of highly-conducting nitrogen-doped ultrananocrystalline diamond films [J].
Bhattacharyya, S ;
Auciello, O ;
Birrell, J ;
Carlisle, JA ;
Curtiss, LA ;
Goyette, AN ;
Gruen, DM ;
Krauss, AR ;
Schlueter, J ;
Sumant, A ;
Zapol, P .
APPLIED PHYSICS LETTERS, 2001, 79 (10) :1441-1443
[5]   Morphology and electronic structure in nitrogen-doped ultrananocrystalline diamond [J].
Birrell, J ;
Carlisle, JA ;
Auciello, O ;
Gruen, DM ;
Gibson, JM .
APPLIED PHYSICS LETTERS, 2002, 81 (12) :2235-2237
[6]  
CARDINALE GF, 1992, J MATER RES, V7, P6
[7]  
CHASIOTIS I, 2000, P SOC PHOTO-OPT INS, V4175, P2
[8]  
CHASIOTIS I, 2001, MATER RES SOC S P, V657, P221
[9]  
CHRISTIANSEN S, 1996, J MATER RES, V11, P8
[10]  
COLES G, 2001, SOC EXP MECH, V1, P176