Oxidation in orthopaedic UHMWPE sterilized by gamma-radiation and ethylene oxide

被引:215
作者
Costa, L
Luda, MP
Trossarelli, L
del Prever, EMB
Crova, M
Gallinaro, P
机构
[1] Univ Turin, Dipartimento Chim Inorgan & Chim Fis, I-10125 Turin, Italy
[2] Univ Turin, Ctr Traumatol Ortoped, Clin Ortoped 1, I-10126 Turin, Italy
[3] Univ Turin, Ctr Traumatol Ortoped, Clin Ortoped 2, I-10126 Turin, Italy
关键词
UHMWPE; sterilization; oxidation; degradation; ageing; FTIR spectroscopy;
D O I
10.1016/S0142-9612(97)00160-9
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Ten new polyethylene prosthetic components (PEs), ethylene oxide (EtO)- and gamma-sterilized, were studied by means of infrared (IR) analysis in order to evaluate oxidation, Using attenuate total reflection infrared spectroscopy the authors demonstrate that all samples show surface oxidation, formed during processing and shaping, related to mechano-degradation. By means of Fourier transform infrared (FTIR) microscopy and derivatization techniques, the EtO-sterilized PEs present different behaviour in comparison to the gamma-radiated. The former show low levels of depth oxidation that could be related to the degradation which occurred during preparation of slices for IR analysis, The gamma-sterilized PEs show higher oxidation levels, variable from sample to sample, on the surface and in the bulk. The authors demonstrate that oxidation is described both by carbonyl species distribution and by hydroperoxide concentration, The hydroperoxides could be responsible for oxidative PEs ageing in in vivo service. The different oxidation levels and distribution could depend on the conditions of gamma-sterilization, in particular on the rate of the dose absorbed, not previously reported for ready-to-implant PEs. Chain scission of gamma-radiated UHMWPE, estimated by IR analysis, results in reduction of molecular weight and consequently in less abrasive resistance. The scheme of UHMWPE oxidation due to gamma-sterilization demonstrates the inhomogeneous distribution of reactive species in PEs responsible for the unpredictable performance in vivo. (C) 1998 Published by Elsevier Science Ltd, All rights reserved.
引用
收藏
页码:659 / 668
页数:10
相关论文
共 37 条
[21]   POLYETHYLENE HYDROPEROXIDE DECOMPOSITION PRODUCTS [J].
LACOSTE, J ;
CARLSSON, DJ ;
FALICKI, S ;
WILES, DM .
POLYMER DEGRADATION AND STABILITY, 1991, 34 (1-3) :309-323
[22]   GAMMA-INITIATED, PHOTO-INITIATED, AND THERMALLY-INITIATED OXIDATION OF LINEAR LOW-DENSITY POLYETHYLENE - A QUANTITATIVE COMPARISON OF OXIDATION-PRODUCTS [J].
LACOSTE, J ;
CARLSSON, DJ .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1992, 30 (03) :493-500
[23]   ULTRA-HIGH-MOLECULAR-WEIGHT POLYETHYLENE - THE MATERIAL AND ITS USE IN TOTAL JOINT IMPLANTS [J].
LI, S ;
BURSTEIN, AH .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1994, 76A (07) :1080-1090
[24]  
Lyons BJ, 1993, ACS SYM SER, V527, P62
[25]  
NEILL PO, 1995, POLYM DEG STAB, V49, P239
[26]   EFFECTS OF RADIATION STERILIZATION ON THE PROPERTIES OF ULTRAHIGH MOLECULAR-WEIGHT POLYETHYLENE [J].
NUSBAUM, HJ ;
ROSE, RM .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1979, 13 (04) :557-576
[27]   TIBIAL HIGH-DENSITY POLYETHYLENE WEAR IN CONFORMING TIBIOFEMORAL PROSTHESES [J].
PLANTEBORDENEUVE, P ;
FREEMAN, MAR .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1993, 75 (04) :630-636
[28]   Gamma sterilization of UHMWPE articular implants: An analysis of the oxidation problem [J].
Premnath, V ;
Harris, WH ;
Jasty, M ;
Merrill, EW .
BIOMATERIALS, 1996, 17 (18) :1741-1753
[29]   POSTIRRADIATION AGING OF ULTRA-HIGH-MOLECULAR-WEIGHT POLYETHYLENE [J].
RIMNAC, CM ;
KLEIN, RW ;
BETTS, F ;
WRIGHT, TM .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1994, 76A (07) :1052-1056
[30]  
SANFORD WM, 1995, 41 ANN M ORTH RES SO