Numerical and experimental study of the circular cracks observed at the contact edges of the indentations of coated systems with soft substrates

被引:41
作者
Souza, RM
Sinatora, A
Mustoe, GGW
Moore, JJ
机构
[1] Univ Sao Paulo, Surface Phenomena Lab, Dept Mech Engn, Polytech Sch, BR-05508900 Sao Paulo, Brazil
[2] Colorado Sch Mines, Div Engn, Golden, CO 80401 USA
[3] Colorado Sch Mines, Adv Coatings & Surface Engn Lab, Golden, CO 80401 USA
基金
巴西圣保罗研究基金会;
关键词
indentation; circular cracks; wear resistant coatings; soft substrates;
D O I
10.1016/S0043-1648(01)00778-5
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this work, the finite element method (FEM) was used, in conjunction with experiments, to study some of the crack patterns observed during the indentation of coated systems. In particular, the study was centered on the array of circular cracks observed close to the contact edge of the spherical indentations of systems with soft substrates. A sequence of steps was considered during the FEM formulation. Initially, the deposition (intrinsic) and thermal (extrinsic) stresses were introduced to account for all the residual stresses present in the deposited films. Later, a loading-unloading sequence was applied on the pre-stressed system, with a maximum normal load of 50N. The FEM also simulated the formation of the circular cracks by considering the presence of fifteen cracks distributed over the film surface and their propagation in the direction perpendicular to the film/substrate interface. Two different types of substrates and two different coatings were analyzed during the experiments. Substrates made of AA 6061 aluminum alloy and AISI 304 stainless steel were coated with (i) titanium nitride (TiN) by unbalanced magnetron sputtering; and (ii) silicon carbide (SiC) by plasma-enhanced chemical vapor deposition. Three thicknesses were studied in each of the four systems, which were later indented with normal loads of 50N, applied by a sphere. The results indicated that, in each case, the array of circular cracks observed close to the contact edge usually develops with a similar inter-crack spacing, which has a strong relation with the film thickness and properties. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:1337 / 1346
页数:10
相关论文
共 31 条
[11]  
Hutchings I. M., 1992, TRIBOLOGY FRICTION W, p[73, 226]
[12]   MIXED-MODE CRACKING IN LAYERED MATERIALS [J].
HUTCHINSON, JW ;
SUO, Z .
ADVANCES IN APPLIED MECHANICS, VOL 29, 1992, 29 :63-191
[13]   ADHESION MEASUREMENTS OF CHEMICALLY VAPOR-DEPOSITED AND PHYSICALLY VAPOR-DEPOSITED HARD COATINGS ON WC-CO SUBSTRATES [J].
JINDAL, PC ;
QUINTO, DT ;
WOLFE, GJ .
THIN SOLID FILMS, 1987, 154 (1-2) :361-375
[14]  
Johnson K.L., 1987, CONTACT MECH, P452
[15]   FINITE-ELEMENT ANALYSIS OF A LAYERED ELASTIC SOLID IN NORMAL CONTACT WITH A RIGID SURFACE [J].
KOMVOPOULOS, K .
JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 1988, 110 (03) :477-485
[16]   Examination of mechanical properties and failure mechanisms of TiN and Ti-TiN multilayer coatings [J].
Ma, K.J. ;
Bloyce, A. ;
Bell, T. .
Surface and Coatings Technology, 1995, 76-77 (1 -3 pt 1) :297-302
[17]   FINITE-ELEMENT ANALYSIS OF ELASTOPLASTIC INDENTATION .2. APPLICATION TO HARD COATINGS [J].
MONTMITONNET, P ;
EDLINGER, ML ;
FELDER, E .
JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 1993, 115 (01) :15-19
[18]   Practical measurement of the residual stress in coatings [J].
Perry, AJ ;
Sue, JA ;
Martin, PJ .
SURFACE & COATINGS TECHNOLOGY, 1996, 81 (01) :17-28
[19]   Residual macroscopic stress in highly preferentially oriented titanium nitride coatings deposited on various steel types [J].
Quaeyhaegens, C ;
Knuyt, G ;
Stals, LM .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1996, 14 (04) :2462-2469
[20]   Diffraction analysis of nonuniform stresses in surface layers: Application to cracked TiN coatings chemically vapor deposited on Mo [J].
Sloof, WG ;
Kooi, BJ ;
Delhez, R ;
deKeijser, TH ;
Mittemeijer, EJ .
JOURNAL OF MATERIALS RESEARCH, 1996, 11 (06) :1440-1457