Grit-blasted titanium femoral stem in cementless primary total hip arthroplasty - A 5-to 10-year multicenter study

被引:42
作者
Delaunay, C [1 ]
Bonnomet, F [1 ]
North, J [1 ]
Jobard, D [1 ]
Cazeau, C [1 ]
Kempf, JF [1 ]
机构
[1] Clin Yvette, F-91160 Longjumeau, France
关键词
primary total hip arthroplasty; cementless stem; grit-blasted titanium; patient selection;
D O I
10.1054/arth.2001.17940
中图分类号
R826.8 [整形外科学]; R782.2 [口腔颌面部整形外科学]; R726.2 [小儿整形外科学]; R62 [整形外科学(修复外科学)];
学科分类号
摘要
A total of 133 cementless primary total hip arthroplasties using the Zweymuller-Alloclassic grit-blasted titanium tapered stem were performed in 3 institutions. The patient cohort was divided into 2 subgroups. nonselected and selected, on the basis of excellent hone stock and age (<65 years old at surgery). Acetabular components were all cementless, and bearing surfaces were all alumina-ceramic on polyethylene, After a 7.3-year average follow-up period (range. 5-10 years), 118 primary femoral replacements in 109 patients could be reviewed fully. Mean age at surgery was 55.7 years (range, 27-84 years). According to the Merle d'Aubigne and Charnley rating system, clinical results were graded excellent and good in 89% of hips and fair in 11%. Radiologically, early subsidence >2 mm could be detected in 4 hips (3.4%). Calcar atrophy and spot welds were noted in 77% and 82% of hips. Femoral osteolysis granuloma was noted in 4 hips (3.4%). There has been no stem fracture and no ceramic head breakage. The survivorship at 10 years with definite femoral aseptic loosening (radiographic failure) as the endpoint was 100% (95% Wilson confidence interval, 78.4%-100%; worst scenario, 95.4%). A significant difference between the nonselected and selected patient subgroups was observed only for early reoperation (P = .03) and proximal stress shielding (P = .01). Press-fitting but not filling the femoral canal with a rough titanium, straight, tapered femoral component represents, at intermediate follow-up, a promising cementless option in primary total hip arthroplasty.
引用
收藏
页码:47 / 54
页数:8
相关论文
共 36 条
[21]  
Lintner F, 1986, J Arthroplasty, V1, P183, DOI 10.1016/S0883-5403(86)80029-8
[22]  
LOVE BRT, 1996, J BONE JOINT SURG S2, V78, P115
[23]  
Merle D'Aubigne R., 1970, REV CHIR ORTHOP, V56, P481
[24]   Loss to follow-up matters [J].
Murray, DW ;
Britton, AR ;
Bulstrode, CJK .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1997, 79B (02) :254-257
[25]  
PERKA C, 1995, METALLPAARUNG METASU, P156
[26]  
RANDELLI G, 1997, J BONE JOINT SURG S2, V79, P238
[27]   In vitro human monocyte response to wear particles of titanium alloy containing vanadium or niobium [J].
Rogers, SD ;
Howie, DW ;
Graves, SE ;
Pearcy, MJ ;
Haynes, DR .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1997, 79B (02) :311-315
[28]   FURTHER EXPERIMENTAL AND CLINICAL EXPERIENCE WITH ALUMINUM-OXIDE ENDOPROSTHESES [J].
SALZER, M ;
ZWEYMULLER, K ;
LOCKE, H ;
ZEIBIG, A ;
STARK, N ;
PLENK, H ;
PUNZET, G .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1976, 10 (06) :847-856
[29]   NEW PROSPECTS FOR A PROLONGED FUNCTIONAL LIFE-SPAN OF ARTIFICIAL HIP JOINTS BY USING MATERIAL COMBINATION POLYETHYLENE-ALUMINUM OXIDE CERAMIC-METAL [J].
SEMLITSCH, M ;
LEHMANN, M ;
WEBER, H ;
DOERRE, E ;
WILLERT, HG .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1977, 11 (04) :537-552
[30]   TITANIUM-ALUMINUM-NIOBIUM ALLOY, DEVELOPMENT FOR BIOCOMPATIBLE, HIGH-STRENGTH SURGICAL IMPLANTS [J].
SEMLITSCH, M ;
STAUB, F ;
WEBER, H .
BIOMEDIZINISCHE TECHNIK, 1985, 30 (12) :334-339