On the improvement of Li charge/discharge cyclability of carbon fibers by making a C/C composite with thermosetting resins

被引:13
作者
Saito, M
Yamaguchi, K
Sekine, K
Takamura, T
机构
[1] Petoca Ltd, Adv Mat Div, Chiyoda Ku, Tokyo 1020094, Japan
[2] Rikkyo Univ, Dept Chem, Toshima Ku, Tokyo 1718501, Japan
关键词
low cyclability; mesophase carbon; Li-ion secondary battery; epoxy resin; phenolic resin;
D O I
10.1016/S0167-2738(00)00364-7
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The charging capacity of the anode of Li-ion secondary batteries is based on the insertion of Li ions into the internal structure of carbonaceous materials, Low temperature mesophase carbon gives rise to an extraordinary capacity up to 900 mAh/g which is over two times that of graphitic carbon now utilized. However, the serious issue of its low cyclability prevents its actual application. Ln an attempt to improve the low cyclability of a mesophase carbon fiber, C/C composites have been prepared with an epoxy or a phenolic resin. The cyclability was found to be considerably improved by making the fiber felt into a C/C composite. The cyclability is dependent on how each individual fiber is bound together by the binder carbon, as well as how the electrical conductivity of the consisting material is increased. Epoxy resin created difficulty in forming a smooth binding but it still gave an improved cyclability as compared to the unbound fiber. Phenolic resin of resol-type showed a very smooth binding, giving rise to a more stabilized cyclability. The importance of the binding of individual active material particles with an electroconductive material for obtaining a long cycle life has been shown. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:199 / 207
页数:9
相关论文
共 14 条
[1]  
COFFEY B, 1995, J ELECTROCHEM SOC, V142, P271
[2]   IRREVERSIBLE CAPACITY OF LITHIUM SECONDARY BATTERY USING MESO-CARBON MICRO BEADS AS ANODE MATERIAL [J].
FUJIMOTO, H ;
MABUCHI, A ;
TOKUMITSU, K ;
KASUH, T .
JOURNAL OF POWER SOURCES, 1995, 54 (02) :440-443
[3]   Impedance study on the electrochemical lithium intercalation into natural graphite powder [J].
Funabiki, A ;
Inaba, M ;
Ogumi, Z ;
Yuasa, S ;
Otsuji, J ;
Tasaka, A .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (01) :172-178
[4]   CHARGE-DISCHARGE CHARACTERISTICS OF MESOPHASE-PITCH-BASED CARBON-FIBERS FOR LITHIUM CELLS [J].
IMANISHI, N ;
KASHIWAGI, H ;
ICHIKAWA, T ;
TAKEDA, Y ;
YAMAMOTO, O ;
INAGAKI, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (02) :315-320
[5]   ELECTROCHEMICAL AND STRUCTURAL STUDIES OF PETROLEUM COKE IN CARBONATE-BASED ELECTROLYTES [J].
JEAN, M ;
DESNOYER, C ;
TRANCHANT, A ;
MESSINA, R .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (07) :2122-2125
[6]   CHARGE-DISCHARGE MECHANISM OF GRAPHITIZED MESOCARBON MICROBEADS [J].
MABUCHI, A ;
FUJIMOTO, H ;
TOKUMITSU, K ;
KASUH, T .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (09) :3049-3051
[7]   CHARGE-DISCHARGE CHARACTERISTICS OF THE MESOCARBON MICROBEADS HEAT-TREATED AT DIFFERENT TEMPERATURES [J].
MABUCHI, A ;
TOKUMITSU, K ;
FUJIMOTO, H ;
KASUH, T .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (04) :1041-1046
[8]   THE ELECTROCHEMICAL-BEHAVIOR OF ALKALI AND ALKALINE-EARTH METALS IN NON-AQUEOUS BATTERY SYSTEMS - THE SOLID ELECTROLYTE INTERPHASE MODEL [J].
PELED, E .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (12) :2047-2051
[9]   New carbon electrodes for secondary lithium batteries [J].
Sandi, G ;
Winans, RE ;
Carrado, KA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (05) :L95-L98
[10]   A MECHANISM OF LITHIUM STORAGE IN DISORDERED CARBONS [J].
SATO, K ;
NOGUCHI, M ;
DEMACHI, A ;
OKI, N ;
ENDO, M .
SCIENCE, 1994, 264 (5158) :556-558