Hydrophobic recovery of polydimethylsiloxane after exposure to partial discharges as a function of crosslink density

被引:137
作者
Hillborg, H
Sandelin, M
Gedde, UW [1 ]
机构
[1] Royal Inst Technol, Dept Polymer Technol, SE-10044 Stockholm, Sweden
[2] ABB Corp Res, Dept High Voltage Engn, SE-72178 Vasteras, Sweden
关键词
polydimethylsiloxane; electrical discharges; hydrophobicity;
D O I
10.1016/S0032-3861(01)00202-6
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polydimethylsiloxanes with different crosslink densities were exposed to corona discharges or GHz air plasma and studied by contact angle measurements, X-ray photoelectron spectroscopy, optical microscopy, scanning electron microscopy and atomic force microscopy. The degree of surface oxidation increased with increasing exposure time with a limiting depth of 100-150 nm. Surface oxidation was faster in more highly crosslinked polymers. Within the oxidised layer, a brittle, microporous silica-like layer with a minimum organic silicone content of 40% gradually developed with increasing exposure time. The strain at which the silica-like layer cracked decreased with increasing dose of corona or air plasma. The hydrophobic recovery following the corona/air plasma exposure occurred at a slow rate by diffusion of oligomers through the microporous but uncracked silica-like layer or at a much higher rate by transport of oligomers through cracks in the silica-like layer. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:7349 / 7362
页数:14
相关论文
共 33 条
[22]  
Leterrier Y, 1997, J POLYM SCI POL PHYS, V35, P1463, DOI 10.1002/(SICI)1099-0488(19970715)35:9<1463::AID-POLB16>3.0.CO
[23]  
2-4
[24]   ON THE AGING OF OXYGEN PLASMA-TREATED POLYDIMETHYLSILOXANE SURFACES [J].
MORRA, M ;
OCCHIELLO, E ;
MAROLA, R ;
GARBASSI, F ;
HUMPHREY, P ;
JOHNSON, D .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1990, 137 (01) :11-24
[25]  
Nielsen J., 1979, J APPL POLYM SCI APP, V35, P223
[26]  
OWEN MJ, 1990, ADV CHEM SER, P705
[27]   PLASMA TREATMENT OF POLYDIMETHYLSILOXANE [J].
OWEN, MJ ;
SMITH, PJ .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1994, 8 (10) :1063-1075
[28]  
SORQVIST T, 1995, P 9 INT S HIGH VOLT, P3234
[29]   THERMAL ANALYSIS OF POLYDIMETHYLSILOXANES .I. THERMAL DEGRADATION IN CONTROLLED ATMOSPHERES [J].
THOMAS, TH ;
KENDRICK, TC .
JOURNAL OF POLYMER SCIENCE PART A-2-POLYMER PHYSICS, 1969, 7 (3PA2) :537-&
[30]   OXIDATIVE DAMAGE AND RECOVERY OF SILICONE-RUBBER SURFACES .1. X-RAY PHOTOELECTRON SPECTROSCOPIC STUDY [J].
TOTH, A ;
BERTOTI, I ;
BLAZSO, M ;
BANHEGYI, G ;
BOGNAR, A ;
SZAPLONCZAY, P .
JOURNAL OF APPLIED POLYMER SCIENCE, 1994, 52 (09) :1293-1307