Hydrophobic recovery of polydimethylsiloxane after exposure to partial discharges as a function of crosslink density

被引:137
作者
Hillborg, H
Sandelin, M
Gedde, UW [1 ]
机构
[1] Royal Inst Technol, Dept Polymer Technol, SE-10044 Stockholm, Sweden
[2] ABB Corp Res, Dept High Voltage Engn, SE-72178 Vasteras, Sweden
关键词
polydimethylsiloxane; electrical discharges; hydrophobicity;
D O I
10.1016/S0032-3861(01)00202-6
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polydimethylsiloxanes with different crosslink densities were exposed to corona discharges or GHz air plasma and studied by contact angle measurements, X-ray photoelectron spectroscopy, optical microscopy, scanning electron microscopy and atomic force microscopy. The degree of surface oxidation increased with increasing exposure time with a limiting depth of 100-150 nm. Surface oxidation was faster in more highly crosslinked polymers. Within the oxidised layer, a brittle, microporous silica-like layer with a minimum organic silicone content of 40% gradually developed with increasing exposure time. The strain at which the silica-like layer cracked decreased with increasing dose of corona or air plasma. The hydrophobic recovery following the corona/air plasma exposure occurred at a slow rate by diffusion of oligomers through the microporous but uncracked silica-like layer or at a much higher rate by transport of oligomers through cracks in the silica-like layer. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:7349 / 7362
页数:14
相关论文
共 33 条
[31]  
TRELOAR LRG, 1975, PHYSICS RUBBER ELAST
[32]   SURFACE STRUCTURAL-CHANGES OF NATURALLY AGED SILICONE AND EPDM COMPOSITE INSULATORS [J].
VLASTOS, AE ;
GUBANSKI, SM .
IEEE TRANSACTIONS ON POWER DELIVERY, 1991, 6 (02) :888-900
[33]  
WROBLE D, 1996, ORGANOSILICON CHEM, V2