Combined effects of environmental vibrations and hygrothermal fatigue on mechanical damage in PEM fuel cells

被引:54
作者
Banan, Roshanak [1 ,2 ]
Bazylak, Aimy [1 ]
Zu, Jean [2 ]
机构
[1] Univ Toronto, Fac Appl Sci & Engn, Dept Mech & Ind Engn, Thermofluids Energy & Adv Mat Lab, Toronto, ON M5S 3G8, Canada
[2] Univ Toronto, Fac Appl Sci & Engn, Dept Mech & Ind Engn, Vibrat Design & Mechatron Lab, Toronto, ON M5S 3G8, Canada
基金
加拿大创新基金会; 加拿大自然科学与工程研究理事会;
关键词
Vibration; Damage propagation; Humidity and temperature cycles; Fatigue; Polymer electrolyte membrane fuel cell; Cohesive elements; POLYMER ELECTROLYTE MEMBRANE; PROTON-EXCHANGE MEMBRANES; GAS-DIFFUSION LAYERS; CATALYST LAYERS; PART I; BEHAVIOR; STACK; DEGRADATION; DURABILITY; DELAMINATION;
D O I
10.1016/j.ijhydene.2014.11.125
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Automotive polymer electrolyte membrane (PEM) fuel cells are exposed to high magnitude road-induced impact loads and vibrations as well as high-level cyclic stresses due to humidity and temperature (hygrothermal) variations. The consequent plastic strain can exacerbate defects and may result in operational failure. In this study, a two-dimensional finite element model based on cohesive zone theory was employed to investigate the combined effects of hygrothermal cycle amplitude and amplitude and frequency of external vibrations on damage propagation. The simultaneous presence of hygrothermal cycles and vibrations severely intensified damage propagation within the expected fuel cell lifetime. Compared with applied vibrations, hygrothermal cycles produced a dominating effect on degradation. Under hygrothermal cycling, membrane cracks experienced more severe propagation compared to delaminations, while vibrations had a more significant effect on delaminations compared to cracks. The presence of a channel offset led to a 2.5-fold increase in delamination length compared to a case with no channel offset. Copyright (C) 2014, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1911 / 1922
页数:12
相关论文
共 50 条
[1]   Use of mechanical tests to predict durability of polymer fuel cell membranes under humidity cycling [J].
Aindow, T. T. ;
O'Neill, J. .
JOURNAL OF POWER SOURCES, 2011, 196 (08) :3851-3854
[2]   The in-plane thermal conductivity and the contact resistance of the components of the membrane electrode assembly in proton exchange membrane fuel cells [J].
Alhazmi, N. ;
Ismail, M. S. ;
Ingham, D. B. ;
Hughes, K. J. ;
Ma, L. ;
Pourkashanian, M. .
JOURNAL OF POWER SOURCES, 2013, 241 :136-145
[3]  
[Anonymous], 2007, D552894A ASTM
[4]  
[Anonymous], 2009, ABAQUS 6 12 DASSAULT
[5]  
[Anonymous], J FUEL CELL SCI TECH
[6]   Effect of mechanical vibrations on damage propagation in polymer electrolyte membrane fuel cells [J].
Banan, Roshanak ;
Bazylak, Aimy ;
Zu, Jean .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (34) :14764-14772
[7]   Measurement of mixed-mode delamination fracture toughness of unidirectional glass/epoxy composites with mixed-mode bending apparatus [J].
Benzeggagh, ML ;
Kenane, M .
COMPOSITES SCIENCE AND TECHNOLOGY, 1996, 56 (04) :439-449
[8]   The effects of mine conditions on the performance of a PEM fuel cell [J].
Bétournay, MC ;
Bonnell, G ;
Edwardson, E ;
Paktunc, D ;
Kaufman, A ;
Lomma, AT .
JOURNAL OF POWER SOURCES, 2004, 134 (01) :80-87
[9]  
Bograchev D., 2007, Int J Hydrogen Energy, V32, P872
[10]   Stress and plastic deformation of MEA in fuel cells - Stresses generated during cell assembly [J].
Bograchev, Danfil ;
Gueguen, Mikael ;
Grandidier, Jean-Claude ;
Martemianov, Serguei .
JOURNAL OF POWER SOURCES, 2008, 180 (01) :393-401