Characterizing composition modulations in InAs/AlAs short-period superlattices

被引:45
作者
Twesten, RD [1 ]
Follstaedt, DM
Lee, SR
Jones, ED
Reno, JL
Millunchick, JM
Norman, AG
Ahrenkiel, SP
Mascarenhas, A
机构
[1] Univ Illinois, Ctr Microanal Mat, Urbana, IL 61801 USA
[2] Sandia Natl Labs, Phys & Chem Sci Ctr, Albuquerque, NM 87185 USA
[3] Univ Michigan, Dept Mat Sci & Engn, Ann Arbor, MI 48109 USA
[4] Natl Renewable Energy Lab, Golden, CO 80401 USA
关键词
D O I
10.1103/PhysRevB.60.13619
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The formation of quantum wires has much interest due to their novel electronic properties which may lead to enhanced optoelectronic device performance and greater photovoltaic efficiencies. One method of forming these structures is through spontaneous lateral modulation found during the epitaxial growth of III/V alloys. In this paper, we report and summarize our investigations on the formation of lateral modulation in the molecular-beam epitaxy grown InAlAs/InP(001) system. This system was grown as a short-period superlattice where n monolayers of InAs are deposited followed by m monolayers of AlAs (with n and m similar to 2) and this sequence is repeated to grow a low strain InAlAs ternary alloy on InP(001) that exhibits lateral modulation. Films were grown under a variety of conditions (growth temperature, effective alloy composition, superlattice period, and growth rate). These films have been extensively analyzed using x-ray diffraction, atomic force microscopy, and transmission electron microscopy (TEM) and microcharacterization, in addition to photon-based spectroscopes. Here we present results of several microstructural characterizations using a wide range of TEM-based techniques, and compare them to results from the other methods to obtain a unified understanding of composition modulation. Two strong points consistently emerge:(1) The lateral modulation wavelength is insensitive to growth temperature and effective alloy composition, but the strength of the lateral modulation is greatest near an effective alloy composition of In0.46Al0.54As, which corresponds to a slightly tensile global strain with respect to InP. (2) The composition variation for the strongly modulated films is as much as 0.38 InAs mole fraction. in addition, for these strongly modulated films, the modulation wave is asymmetric showing strongly peaked, narrower InAs-rich regions separated by flat AlAs-rich regions. We discuss these results and their possible implications in addition to detailing the techniques used to obtain them. [S0163-1829(99)10743-4].
引用
收藏
页码:13619 / 13635
页数:17
相关论文
共 46 条
[1]   Laterally modulated composition profiles in AlAs/InAs short-period superlattices [J].
Ahrenkiel, SP ;
Norman, AG ;
Al-Jassim, MM ;
Mascarenhas, A ;
Mirecki-Millunchick, J ;
Twesten, RD ;
Lee, SR ;
Follstaedt, DM ;
Jones, ED .
JOURNAL OF APPLIED PHYSICS, 1998, 84 (11) :6088-6094
[2]  
[Anonymous], ADV XRAY ANAL
[3]   INTERFACE MORPHOLOGY DEVELOPMENT DURING STRESS-CORROSION CRACKING .1. VIA SURFACE DIFFUSION [J].
ASARO, RJ ;
TILLER, WA .
METALLURGICAL TRANSACTIONS, 1972, 3 (07) :1789-&
[4]   ABSORPTIVE FORM-FACTORS FOR HIGH-ENERGY ELECTRON-DIFFRACTION [J].
BIRD, DM ;
KING, QA .
ACTA CRYSTALLOGRAPHICA SECTION A, 1990, 46 :202-208
[5]   ON SPINODAL DECOMPOSITION [J].
CAHN, JW .
ACTA METALLURGICA, 1961, 9 (09) :795-801
[6]   GAXIN1-XAS MULTIPLE-QUANTUM-WIRE LASERS GROWN BY THE STRAIN-INDUCED LATERAL-LAYER ORDERING PROCESS [J].
CHOU, ST ;
CHENG, KY ;
CHOU, LJ ;
HSIEH, KC .
APPLIED PHYSICS LETTERS, 1995, 66 (17) :2220-2222
[7]   GROWTH OF GAXIN1-XAS QUANTUM-WIRE HETEROSTRUCTURES BY THE STRAIN-INDUCED LATERAL-LAYER ORDERING PROCESS [J].
CHOU, ST ;
HSIEH, KC ;
CHENG, KY ;
CHOU, LJ .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1995, 13 (02) :650-652
[8]  
CULLIS AG, 1995, MICROSCOPY SEMICONDU
[9]   KINETIC-MODEL OF ELEMENT-III SEGREGATION DURING MOLECULAR-BEAM EPITAXY OF III-III'-IV-SEMICONDUCTOR COMPOUNDS [J].
DEHAESE, O ;
WALLART, X ;
MOLLOT, F .
APPLIED PHYSICS LETTERS, 1995, 66 (01) :52-54
[10]   DISLOCATION-FREE STRANSKI-KRASTANOW GROWTH OF GE ON SI(100) [J].
EAGLESHAM, DJ ;
CERULLO, M .
PHYSICAL REVIEW LETTERS, 1990, 64 (16) :1943-1946