A systematic study of the defects in ZnO has been performed. The two commonly observed levels (L1, L2), located at around 0.15 and 0.24 eV under the conduction band, have been identified as native defects. The deep level transient spectroscopy depth profiling technique is applied on multilayer-chip-type ZnO varistors to determine the distribution profiles of these two levels. With higher densities near the grain boundary, L2 is unlikely to be zinc interstitials as some previous studies have assigned, Both L1 and L2 show no apparent correlation with the device degradation process. Instead, a complex defect or interface trap, related to impurities in the starting material, exhibits a much stronger correlation with the ZnO varistor's stability. (C) 1996 American Institute of Physics.
引用
收藏
页码:526 / 528
页数:3
相关论文
共 10 条
[1]
DEEP-LEVEL TRANSIENT SPECTROSCOPY OF ZINC-OXIDE VARISTORS DOPED WITH ALUMINUM-OXIDE AND OR SILVER-OXIDE [J].
FAN, JW ;
FREER, R .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (10) :2663-2668
[2]
APPLICATION OF ZINC-OXIDE VARISTORS [J].
GUPTA, TK .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (07) :1817-1840
[3]
GUPTA TK, 1985, J MATER SCI, V20, P3847
[4]
FAST CAPACITANCE TRANSIENT APPARATUS - APPLICATION TO ZNO AND O CENTERS IN GAP PARANORMAL JUNCTIONS [J].
LANG, DV .
JOURNAL OF APPLIED PHYSICS, 1974, 45 (07) :3014-3022
[5]
EXTENDED BULK DEFECTS INDUCED BY LOW-ENERGY IONS DURING PARTIALLY IONIZED BEAM DEPOSITION [J].
LEE, WI ;
WONG, J ;
BORREGO, JM ;
LU, TM .
JOURNAL OF APPLIED PHYSICS, 1988, 64 (04) :2206-2208
[6]
PHASE IDENTIFICATION AND ELECTRICAL-PROPERTIES IN ZNO-GLASS VARISTORS [J].
LEE, YS ;
TSENG, TY .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (06) :1636-1640
[7]
PHYSICS OF METAL-OXIDE VARISTORS [J].
LEVINSON, LM ;
PHILIPP, HR .
JOURNAL OF APPLIED PHYSICS, 1975, 46 (03) :1332-1341
[8]
THE DEEP LEVEL TRANSIENT SPECTROSCOPY STUDIES OF A ZNO VARISTOR AS A FUNCTION OF ANNEALING [J].
ROHATGI, A ;
PANG, SK ;
GUPTA, TK ;
STRAUB, WD .
JOURNAL OF APPLIED PHYSICS, 1988, 63 (11) :5375-5379
[9]
DEFECT CLUSTERS IN ZINC-OXIDE [J].
SIMPSON, JC ;
CORDARO, JF .
JOURNAL OF APPLIED PHYSICS, 1990, 67 (11) :6760-6763
[10]
ELECTRICAL-PROPERTIES OF MULTILAYER-CHIP ZNO VARISTORS IN A MOIST-AIR ENVIRONMENT [J].
YEN, AJ ;
LEE, YS ;
TSENG, TY .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (11) :3006-3011