Thermal conductivity of negative-thermal-expansion oxide, Zr1-xYxW2O8 (x-0.00, 0.01)-temperature dependence and effect of structural phase transition

被引:25
作者
Hashimoto, T
Kuwahara, J
Yoshida, T
Nashimoto, M
Takahashi, Y
Takahashi, K
Morito, Y
机构
[1] Nihon Univ, Coll Humanities & Sci, Dept Integrated Sci Phys & Biol, Setagaya Ku, Tokyo 1568550, Japan
[2] Moritex Corp, Shibuya Ku, Tokyo 1500001, Japan
[3] Moritex Corp, Yaita Factory, Yaita, Tochigi 3292135, Japan
[4] Chuo Univ, Fac Sci & Engn, Dept Appl Chem, Bunkyo Ku, Tokyo 1128551, Japan
关键词
heat conduction; phase transitions; thermal expansion;
D O I
10.1016/j.ssc.2004.05.001
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
The temperature dependence of the thermal conductivity of the negative-thermal-expansion oxide, ZrW2O8, was evaluated. The room temperature thermal conductivities of ZrW2O8 and Zr0.99Y0.01W2O8 were approximately 0.80 and 0.65 W m(-1) K-1, respectively, which are lower than those of other functional oxides. It was revealed that the mechanism of thermal resistance is phonon-phonon scattering, which is affected by the phase transition at approximately 420 K. The different thermal conductivities of Zr0.99Y0.01W2O8 and ZrW2O8, suggests that Y3+ works as a scattering center for thermal conduction. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:217 / 221
页数:5
相关论文
共 23 条
[11]   THE POSSIBILITY OF HIGH-TEMPERATURE HEAT-CAPACITY MEASUREMENTS BY DIFFERENTIAL SCANNING CALORIMETRY [J].
KAMIMOTO, M .
INTERNATIONAL JOURNAL OF THERMOPHYSICS, 1990, 11 (02) :305-314
[12]   SOME PROBLEMS IN THE PREPARATION OF SUPERCONDUCTING OXIDE-FILMS ON CERAMIC SUBSTRATES [J].
KOINUMA, H ;
KAWASAKI, M ;
HASHIMOTO, T ;
NAGATA, S ;
KITAZAWA, K ;
FUEKI, K ;
MASUBUCHI, K ;
KUDO, M .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 1987, 26 (05) :L763-L765
[13]   Negative thermal expansion from 0.3 to 1050 Kelvin in ZrW2O8 [J].
Mary, TA ;
Evans, JSO ;
Vogt, T ;
Sleight, AW .
SCIENCE, 1996, 272 (5258) :90-92
[14]   Press-free preparation method of dense negative-thermal-expansion oxide, Zr1-xYxW2O8-δ (x=0.00-0.02) ceramic using reactive sintering [J].
Morito, Y ;
Takahashi, K ;
Wang, SR ;
Abe, H ;
Katoh, A ;
Hashimoto, T .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2002, 110 (09) :807-812
[15]  
NAKAMURA T, 1997, PEROVSKITE RELATED C, V32, P37
[16]   Preparation of dense ZrO2/ZrW2O8 cosintered ceramics with controlled thermal expansion coefficients [J].
Niwa, E ;
Wakamiko, S ;
Ichikawa, T ;
Wang, SR ;
Hashimoto, T ;
Takahashi, K ;
Morito, Y .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2004, 112 (1305) :271-275
[17]   THERMAL CONDUCTIVITY OF BEO SINGLE CRYSTALS [J].
SLACK, GA ;
AUSTERMAN, SB .
JOURNAL OF APPLIED PHYSICS, 1971, 42 (12) :4713-+
[18]   THERMAL CONTRACTION [J].
SLEIGHT, AW .
ENDEAVOUR, 1995, 19 (02) :64-68
[19]   Compounds that contract on heating [J].
Sleight, AW .
INORGANIC CHEMISTRY, 1998, 37 (12) :2854-2860
[20]  
Takahashi Y., 1984, International Journal of Thermophysics, V5, P41, DOI 10.1007/BF00502078