Synthesis of aluminum oxide coating with carbon nanotube reinforcement produced by chemical vapor deposition for improved fracture and wear resistance

被引:94
作者
Keshri, Anup K. [1 ,2 ]
Huang, Jun [3 ]
Singh, Virendra [4 ,5 ]
Choi, Wonbong [3 ]
Seal, Sudipta [4 ,5 ]
Agarwal, Arvind [1 ,2 ]
机构
[1] Florida Int Univ, Plasma Forming Lab, Miami, FL 33174 USA
[2] Florida Int Univ, High Temp Tribol Lab, Miami, FL 33174 USA
[3] Florida Int Univ, Nanomat & Device Lab, Miami, FL 33174 USA
[4] Univ Cent Florida, AMPAC, Orlando, FL 32816 USA
[5] Univ Cent Florida, Nanosci Technol Ctr, Orlando, FL 32816 USA
关键词
CERAMIC-MATRIX; TRIBOLOGICAL BEHAVIOR; MECHANICAL-PROPERTIES; NANOCOMPOSITE; POLYMER; SINGLE;
D O I
10.1016/j.carbon.2009.08.046
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Chemical vapor deposition (CVD) was used to achieve a homogeneous dispersion of carbon nanotubes (CNTs) on aluminum oxide (Al2O3) powder. This powder was plasma sprayed onto a steel substrate to produce a 96% dense Al2O3 coating with CNT reinforcement. Addition of 1.5 wt.% CNTs showed a 24% increase in the relative fracture toughness of the composite coating. The improvement in the fracture toughness is attributed to uniform dispersion of CNTs and toughening mechanism such as CNT bridging, crack deflection and strong interaction between CNT/Al2O3 interfaces. Wear and friction behavior of the CNT reinforced Al2O3 coating under dry sliding condition was investigated by ball-on-disk tribometer. With the increasing normal loads from 10 to 50 N, the wear volume loss and coefficient of friction of the coating increased, owing to transition from the mild to severe wear. Wear resistance of the Al2O3-CNT composite coating improved by similar to 27% at 50 N. Coefficient of friction at 50 N was dependent on the competing phenomena of wear debris generation and graphitization due to pressure. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:431 / 442
页数:12
相关论文
共 35 条
[21]   Effect of CNT distribution on tribological behavior of alumina-CNT composites [J].
Lim, DS ;
You, DH ;
Choi, HJ ;
Lim, SH ;
Jang, H .
WEAR, 2005, 259 (1-6) :539-544
[22]   Elastic properties of single and multilayered nanotubes [J].
Lu, JP .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1997, 58 (11) :1649-1652
[23]   Fabrication of carbon nanotube reinforced alumina matrix nanocomposite by sol-gel process [J].
Mo, CB ;
Cha, SI ;
Kim, KT ;
Lee, KH ;
Hong, SH .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 395 (1-2) :124-128
[24]  
OULDRIANE SD, 2006, CARBON, V44, P814
[25]   Flexural deflection as a measure of van der Waals interaction forces in the CNT array [J].
Pipes, RB ;
Hubert, P ;
Salvetat, JP ;
Zalamea, L .
COMPOSITES SCIENCE AND TECHNOLOGY, 2006, 66 (09) :1125-1131
[26]   Aqueous colloidal processing of single-wall carbon nanotubes and their composites with ceramics [J].
Poyato, R ;
Vasiliev, AL ;
Padture, NP ;
Tanaka, H ;
Nishimura, T .
NANOTECHNOLOGY, 2006, 17 (06) :1770-1777
[27]   Mechanical properties of carbon nanotubes: a fiber digest for beginners [J].
Salvetat-Delmotte, JP ;
Rubio, A .
CARBON, 2002, 40 (10) :1729-1734
[28]   Mechanical behavior of polymer and ceramic matrix nanocomposites [J].
Siegel, RW ;
Chang, SK ;
Ash, BJ ;
Stone, J ;
Ajayan, PM ;
Doremus, RW ;
Schadler, LS .
SCRIPTA MATERIALIA, 2001, 44 (8-9) :2061-2064
[29]   Influence of dispersion states of carbon nanotubes on physical properties of epoxy nanocomposites [J].
Song, YS ;
Youn, JR .
CARBON, 2005, 43 (07) :1378-1385
[30]   Development of a dispersion process for carbon nanotubes in ceramic matrix by heterocoagulation [J].
Sun, J ;
Gao, L .
CARBON, 2003, 41 (05) :1063-1068