Viscoelastic and dielectric behaviour of thin films made from siloxane-containing poly(oxadiazole-imide)s

被引:54
作者
Damaceanu, Mariana-Dana [1 ]
Musteata, Valentina-Elena [1 ]
Cristea, Mariana [1 ]
Bruma, Maria [1 ]
机构
[1] Petru Poni Inst Macromol Chem, Iasi 700487, Romania
关键词
Dielectric properties; Poly(oxadiazole-imide)s; Relaxation; Tensile properties; Viscoelastic properties; ELECTROCHEMICAL PROPERTIES; RELAXATION; POLYIMIDE; GLASS; POLARIZATION; SILICON; TEMPERATURE; COPOLYMERS; SURFACE;
D O I
10.1016/j.eurpolymj.2010.01.020
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Siloxane-containing poly(oxadiazole-imide)s were prepared by polycondensation reaction of two aromatic diamino-oxadiazoles with a dianhydride containing tetramethylsiloxane moiety. Free-standing flexible films having good mechanical properties were made therefrom. The polyimides exhibited high thermal stability with initial decomposition temperature being above 440 degrees C and glass transition in the range of 165-183 degrees C. The dielectric constant values, measured at room temperature and in the frequency domain of 1 Hz-1 MHz, are in the range of 2.69-2.90, being significantly lower in comparison with that of Kapton HN (R) film, whose dielectric constant values ranged from 3.13 to 3.24. The dielectric loss values are low, in the same range with those of Kapton HN (R). The dielectric spectroscopy data corroborated with the dynamo-mechanical analysis ones showed distinct sub-glass transitions for these polymers: gamma relaxations with activation energies of 44 and 45 kJ/mol, and beta relaxation with an activation energy of 107 kJ/mol. The dielectric properties are discussed in comparison with those of Kapton HN (R) film measured under the same conditions. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1049 / 1062
页数:14
相关论文
共 52 条
[31]   Low-dielectric, nanoporous polyimide films prepared from PEO-POSS nanoparticles [J].
Lee, YJ ;
Huang, JM ;
Kuo, SW ;
Chang, FC .
POLYMER, 2005, 46 (23) :10056-10065
[32]  
MACEDO PB, 1972, PHYS CHEM GLASSES, V13, P171
[33]   Surface characterization and adhesive properties of poly(imidesiloxane) copolymers containing multiple siloxane segment lengths [J].
Mahoney, CM ;
Gardella, JA ;
Rosenfeld, JC .
MACROMOLECULES, 2002, 35 (13) :5256-5266
[34]   Low dielectric constant polymers for microelectronics [J].
Maier, G .
PROGRESS IN POLYMER SCIENCE, 2001, 26 (01) :3-65
[35]  
Mercer F. W., 1993, High Performance Polymers, V5, P69, DOI 10.1088/0954-0083/5/1/007
[36]   Classification of secondary relaxation in glass-formers based on dynamic properties [J].
Ngai, KL ;
Paluch, M .
JOURNAL OF CHEMICAL PHYSICS, 2004, 120 (02) :857-873
[37]   Conductivity and dielectric relaxation in sodium borosulfate glasses [J].
Pal, Inder ;
Agarwal, Ashish ;
Sanghi, Sujata ;
Sheoran, Anshu ;
Ahlawat, Neetu .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 472 (1-2) :40-45
[38]   Effect of polyimides with different ratios of para- to meta- analogous fluorinated diamines on relaxation process [J].
Qu, WL ;
Ko, TM ;
Vora, RH ;
Chung, TS .
POLYMER, 2001, 42 (15) :6393-6401
[39]   ANISOTROPIC PROPERTIES OF HIGH-TEMPERATURE POLYIMIDE THIN-FILMS - DIELECTRIC AND THERMAL-EXPANSION BEHAVIORS [J].
REE, M ;
CHEN, KJ ;
KIRBY, DP ;
KATZENELLENBOGEN, N ;
GRISCHKOWSKY, D .
JOURNAL OF APPLIED PHYSICS, 1992, 72 (05) :2014-2021
[40]  
ROSENFELD J, 1996, POLYM MAT ENCY, V8, P6198