The effect of reaction time and temperature during heterogenous alkali deacetylation on degree of deacetylation and molecular weight of resulting chitosan

被引:79
作者
Tsaih, ML
Chen, RH [1 ]
机构
[1] Deh Yu Coll Nursing & Management, Chilung, Taiwan
[2] Natl Taiwan Ocean Univ, Dept Food Sci, Chilung, Taiwan
关键词
chitosan; heterogenous alkali deacetylation; reaction rate; reaction order; rate constant; molecular weight; degree of deacetylation;
D O I
10.1002/app.11986
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The objective of the study is to elucidate the effect of reaction time and temperature during heterogenous alkali reaction on degree of deacetylation (DD) and molecular weight (MW) of the resulting chitosans, and to establish the reaction conditions to obtain desired DD and MW chitosan products. Chitin was extracted from red shrimp process waste. DDs and MWs were determined by infrared spectroscopy (IR) and static light scattering, respectively. The results are as follow: The DD and MW of chitin obtained were 31.9% and 5637 kDa, respectively. The DD of the resulting chitosan increased along with reaction time and/or reaction temperature. The DDs of the resulting chitosan that were obtained from 140degreesC were higher than those reacted at 99degreesC. The highest DD of the resulting chitosans after alkali deacetylation at 99 and 140degreesC were 92.2 and 95.1%, respectively. The DDs of chitosans increased fast at the beginning of reaction process then slowed over time. The reaction rate and rate constant of the deacetylation reaction decreased with increasing DD of the reactant. The MWs of chitosans decreased along with the deacetylation time. MW of those chitosans reacted at 140degreesC are smaller than those at 99degreesC. The rate of chitosan degradation was above 43.6%/h in the initial stage, then decreased to about 20%/h. The degradation rate constants raised substantially in the late stage. (C) 2003 Wiley Periodicals, Inc.
引用
收藏
页码:2917 / 2923
页数:7
相关论文
共 53 条
[1]   SOLUTION PROPERTIES OF CHITOSANS - CONFORMATION AND CHAIN STIFFNESS OF CHITOSANS WITH DIFFERENT DEGREES OF N-ACETYLATION [J].
ANTHONSEN, MW ;
VARUM, KM ;
SMIDSROD, O .
CARBOHYDRATE POLYMERS, 1993, 22 (03) :193-201
[2]   IMPROVED METHOD FOR IR DETERMINATION OF THE DEGREE OF N-ACETYLATION OF CHITOSAN [J].
BAXTER, A ;
DILLON, M ;
TAYLOR, KDA ;
ROBERTS, GAF .
INTERNATIONAL JOURNAL OF BIOLOGICAL MACROMOLECULES, 1992, 14 (03) :166-169
[3]   INFLUENCE OF MANUFACTURING VARIABLES ON CHARACTERISTICS AND EFFECTIVENESS OF CHITOSAN PRODUCTS .1. CHEMICAL COMPOSITION, VISCOSITY, AND MOLECULAR-WEIGHT DISTRIBUTION OF CHITOSAN PRODUCTS [J].
BOUGH, WA ;
SALTER, WL ;
WU, ACM ;
PERKINS, BE .
BIOTECHNOLOGY AND BIOENGINEERING, 1978, 20 (12) :1931-1943
[4]   Heterogeneous N-deacetylation of chitin in alkaline solution [J].
Chang, KLB ;
Tsai, G ;
Lee, J ;
Fu, WR .
CARBOHYDRATE RESEARCH, 1997, 303 (03) :327-332
[5]  
Chen R. H., 2000, INT J COSMETIC SCI, V22, P349, DOI [10.1111/j.1467-2494.2000.00036.x, DOI 10.1111/J.1467-2494.2000.00036.X]
[6]  
Chen RH, 1996, CARBOHYD POLYM, V29, P353
[7]   RELATIONSHIPS BETWEEN THE CHAIN FLEXIBILITIES OF CHITOSAN MOLECULES AND THE PHYSICAL-PROPERTIES OF THEIR CASTED FILMS [J].
CHEN, RH ;
LIN, JH ;
YANG, MH .
CARBOHYDRATE POLYMERS, 1994, 24 (01) :41-46
[8]  
Chen RH, 1997, J APPL POLYM SCI, V66, P161, DOI 10.1002/(SICI)1097-4628(19971003)66:1<161::AID-APP19>3.0.CO
[9]  
2-4
[10]   Effects of chain flexibility of chitosan molecules on the preparation, physical, and release characteristics of the prepared capsule [J].
Chen, RH ;
Tsaih, ML ;
Lin, WC .
CARBOHYDRATE POLYMERS, 1996, 31 (03) :141-148