Synthesis and characterization of nano-crystalline CVD diamond film on pure titanium using Ar/CH4/H2 gas mixture

被引:30
作者
Askari, S. J. [1 ]
Akhtar, F. [1 ]
Chen, G. C. [1 ]
He, Q. [1 ]
Wang, F. Y. [1 ]
Meng, X. M. [1 ]
Lu, F. X. [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Dept High Tech Thin Films, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
chemical vapor deposition; nano-crystalline diamond thin film; tribology; pure titanium substrate;
D O I
10.1016/j.matlet.2006.08.033
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Titanium and Ti alloys have poor tribological properties and deposition of a well adherent diamond coating is a promising way to solve this problem. But diamond film deposition on pure titanium and Ti alloys is always difficult due to the high diffusion coefficient of carbon in Ti, the large mismatch in their thermal expansion coefficients, the complex nature of the interlayer formed during diamond deposition, and the difficulty of achieving very high nucleation density. A nano-crystalline diamond (NCD) film can resolve Ti and Ti alloys weak tribological performance due to its smooth surface. A well-adhered NCD film was successfully deposited on pure Ti substrate by using a microwave plasma assisted chemical vapor deposition (M\ATCVD) system in the environment of Ar, CH4 and H-2 gases at a moderate temperature. Detailed experimental results on the preparation, characterization and successful deposition of the NCD film on pure Ti are discussed. (c) 2006 Elsevier B.V All rights reserved.
引用
收藏
页码:2139 / 2142
页数:4
相关论文
共 22 条
[1]  
ASKARI SJ, IN PRESS J U SCI TEC, V13
[2]   TRIBOLOGICAL PROPERTIES OF TITANIUM-ALLOYS [J].
BUDINSKI, KG .
WEAR, 1991, 151 (02) :203-217
[3]  
BUDINSKI KG, 1991, C P ASME, P289
[4]   Characterization of ballas diamond depositions [J].
Bühlmann, S ;
Blank, E ;
Haubner, R ;
Lux, B .
DIAMOND AND RELATED MATERIALS, 1999, 8 (2-5) :194-201
[5]   Mechanical properties and quality of diamond films synthesized on Ti-6Al-4V alloy using the microwave plasmas of CH4/H2 and CO/H2 systems [J].
Catledge, SA ;
Vohra, YK .
JOURNAL OF APPLIED PHYSICS, 1998, 83 (01) :198-204
[6]   Tribological performance of diamond-coated Ti-6Al-4V alloy with respect to diamond characteristics [J].
De Barros, MI ;
Vandenbulcke, L ;
Fontaine, J ;
Farges, G ;
Vayer, M ;
Erre, R .
SURFACE & COATINGS TECHNOLOGY, 2000, 127 (2-3) :193-202
[7]   Tribological properties of nanocrystalline diamond films [J].
Erdemir, A ;
Fenske, GR ;
Krauss, AR ;
Gruen, DM ;
McCauley, T ;
Csencsits, RT .
SURFACE & COATINGS TECHNOLOGY, 1999, 120 :565-572
[8]   Effects of pre-treatments and interlayers on the nucleation and growth of diamond coatings on titanium substrates [J].
Fu, YQ ;
Yan, B ;
Loh, NL .
SURFACE & COATINGS TECHNOLOGY, 2000, 130 (2-3) :173-185
[9]   SCALING LAWS FOR DIAMOND CHEMICAL-VAPOR-DEPOSITION .2. ATOMIC-HYDROGEN TRANSPORT [J].
GOODWIN, DG .
JOURNAL OF APPLIED PHYSICS, 1993, 74 (11) :6895-6906
[10]   Nanocrystalline diamond films [J].
Gruen, DM .
ANNUAL REVIEW OF MATERIALS SCIENCE, 1999, 29 :211-259