Effects of thermal treatment on the properties of ZnO films deposited on MgO-buffered Si substrates

被引:20
作者
Chen, SJ
Liu, YC
Ma, JG
Lu, YM
Zhang, JY
Shen, DZ
Fan, XW
机构
[1] Chinese Acad Sci, Key Lab Excited State Proc, Changchun Inst Opt Fine Mech & Phys, Changchun 130021, Peoples R China
[2] NE Normal Univ, Adv Ctr Optoelect Funct Mat Res, Changchun 130024, Peoples R China
基金
中国国家自然科学基金;
关键词
crystal structure; photoluminescence; x-ray diffraction; physical vapor deposition processes; zinc compounds; semiconducting II-VI materials;
D O I
10.1016/S0022-0248(03)01144-8
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
High quality ZnO thin films have been grown on Si (100) substrates with MgO buffer layers. An electron beam evaporation technique was used to grow MgO buffer layer on Si substrates followed by a magnetron sputtering process to deposit Zn films on the MgO-buffered Si substrates, next, a two-step annealing process was employed to oxidize the Zn films to form ZnO. The effects of the annealing temperature on the photoluminescence (PL) and orientation of ZnO nanocrystalline thin films were studied. For ZnO films annealed between 400degreesC and 700degreesC in an O-2 ambient, the quality of the ZrO films was improved with increasing annealing temperature. However, as the annealing temperature was increased to over 800degreesC, the ZnO film under-went a phase transformation from ZnO to a MgxZn1-xO alloy, where the x value in the alloy increased with increasing annealing temperature. The MgxZn1-xO alloy films were characterized by X-ray diffraction (XRD), photoluminescence (PL)and reflection spectra. XRD results show that the MgxZn1-xO alloy films maintain the hexagonal structure with a lattice constant close to that of ZnO. In films with Mg incorporation, intense ultraviolet band edge photoluminescence was observed at room temperature. The photoluminescence (PL) spectra show that MgxZn1-xO alloy has a wide band gap with a large exciton binding energy of 53 meV. The band gap of the MgxZn1-xO alloy shifts to higher energy with increasing annealing temperature. The blue-shift of the fundamental band gap of the alloy annealed at 1000degreesC is estimated to be similar to300meV. (C) 2003 Published by Elsevier Science B.V.
引用
收藏
页码:86 / 91
页数:6
相关论文
共 21 条
[1]  
AITA CR, 1980, P IEEE ULTR S, P795
[2]  
ARONOVICH J, 1979, J VAC SCI TECHNOL, V16, P994
[4]   Photoluminescence and ultraviolet lasing of polycrystalline ZnO thin films prepared by the oxidation of the metallic Zn [J].
Cho, SL ;
Ma, J ;
Kim, YK ;
Sun, Y ;
Wong, GKL ;
Ketterson, JB .
APPLIED PHYSICS LETTERS, 1999, 75 (18) :2761-2763
[5]   EXCITONS AND ABSORPTION EDGE OF ZNO [J].
DIETZ, RE ;
THOMAS, DG ;
HOPFIELD, JJ .
JOURNAL OF APPLIED PHYSICS, 1961, 32 :2282-&
[6]   EPITAXIAL MGO ON GAAS(111) AS A BUFFER LAYER FOR Z-CUT EPITAXIAL LITHIUM-NIOBATE [J].
FORK, DK ;
ANDERSON, GB .
APPLIED PHYSICS LETTERS, 1993, 63 (08) :1029-1031
[7]   MGO EPITAXIAL THIN-FILMS ON (100) GAAS AS A SUBSTRATE FOR THE GROWTH OF ORIENTED PBTIO3 [J].
HSU, WY ;
RAJ, R .
APPLIED PHYSICS LETTERS, 1992, 60 (25) :3105-3107
[8]  
Joint Committee Power Diffraction Standards, 361451 JOINT COMM PO
[9]   STUDIES OF OPTIMUM CONDITIONS FOR GROWTH OF RF-SPUTTERED ZNO FILMS [J].
KHURIYAKUB, BT ;
KINO, GS ;
GALLE, P .
JOURNAL OF APPLIED PHYSICS, 1975, 46 (08) :3266-3272
[10]   Temperature-dependent micro-photoluminescence of individual CdSe self-assembled quantum dots [J].
Kim, JC ;
Rho, H ;
Smith, LM ;
Jackson, HE ;
Lee, S ;
Dobrowolska, M ;
Furdyna, JK .
APPLIED PHYSICS LETTERS, 1999, 75 (02) :214-216