The corrosion of ceramic-matrix composites

被引:16
作者
Colomban, P
机构
[1] Off Natl Etud & Rech Aerosp, OM, F-92322 Chatillon, France
[2] CNRS, LASIR, F-94320 Thiais, France
来源
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2 | 1997年 / 251-2卷
关键词
ceramic-matrix composites; external corrosion; internal corrosion; proton; sodium molten salts; LAS; GAS; celsian; cordierite; Al2TiO5; mullite; nasicon; NLM202 Nicalon (TM) SiC fibre;
D O I
10.4028/www.scientific.net/MSF.251-254.833
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ceramic matrix composites could replace existing metals and alloys in aircraft, naval engine parts or heat exchanged systems because of their low density and high thermostability. These composites are promising materials for long-life applications if the metastable state of the composite is preserved during the synthesis and on working atmospheres without deleterious evolution of the fibre, the matrix and of the fibre-matrix interface, The review begins with a brief recall on the corrosion of ceramics able to be used in composites (SiC, Si3N4, AlN, BN, aluminosilicates, C). The main sources of corrosion in combustion environment (proton, sodium ion) are discussed. A comparison is made with long-term corrosion at room-temperature. Examples of the different corrosion mechanisms observed for Nicalon NLM202 fibre glass-ceramic or ceramic (LAS, GAS, celsian, cordierite, Al2TiO5, mullite, Nasicon) matrix composites developed at ONERA are presented : ion exchange, grain boundary dissolution, fluxing, favourable and unfavourable fibre-matrix reaction, enhanced corrosion by prior fibre-matrix reaction.
引用
收藏
页码:833 / 844
页数:12
相关论文
共 46 条
[1]  
[Anonymous], 1990, HDB CERAMICS COMPOSI
[2]   CARBON-CARBON COMPOSITES - OXIDATION BEHAVIOR AND COATINGS PROTECTION [J].
BACOS, MP .
JOURNAL DE PHYSIQUE IV, 1993, 3 (C7) :1895-1903
[3]  
BACOS MP, 1995, HIGH TEMPERATURE CER, V1, P437
[4]  
BALDUS HP, 1995, HIGH TEMPERATURE CER, V2, P75
[5]  
BAXTER DJ, 1993, J MATER SCI LETT, V12, P1533
[6]   CORROSION OF CORDIERITE CERAMICS BY SODIUM-SULFATE AT 1000-DEGREES-C [J].
BIANCO, R ;
JACOBSON, N .
JOURNAL OF MATERIALS SCIENCE, 1989, 24 (08) :2903-2910
[7]  
BRUNETON E, 1992, THESIS PARIS
[8]  
BRUNETON E, 1993, J PHYSIQUE, P1937
[9]   HYDROGEN-BONDING IN HYDROGEN-SUBSTITUTED LITHIUM ALUMINOSILICATES [J].
COLOMBAN, P .
JOURNAL OF MOLECULAR STRUCTURE, 1992, 270 :407-416
[10]   Sol-gel mullite matrix-SiC and -mullite 2D woven fabric composites with or without zirconia containing interphase: Elaboration and properties [J].
Colomban, P ;
Bruneton, E ;
Lagrange, JL ;
Mouchon, E .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1996, 16 (02) :301-314