The corrosion of ceramic-matrix composites

被引:16
作者
Colomban, P
机构
[1] Off Natl Etud & Rech Aerosp, OM, F-92322 Chatillon, France
[2] CNRS, LASIR, F-94320 Thiais, France
来源
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2 | 1997年 / 251-2卷
关键词
ceramic-matrix composites; external corrosion; internal corrosion; proton; sodium molten salts; LAS; GAS; celsian; cordierite; Al2TiO5; mullite; nasicon; NLM202 Nicalon (TM) SiC fibre;
D O I
10.4028/www.scientific.net/MSF.251-254.833
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ceramic matrix composites could replace existing metals and alloys in aircraft, naval engine parts or heat exchanged systems because of their low density and high thermostability. These composites are promising materials for long-life applications if the metastable state of the composite is preserved during the synthesis and on working atmospheres without deleterious evolution of the fibre, the matrix and of the fibre-matrix interface, The review begins with a brief recall on the corrosion of ceramics able to be used in composites (SiC, Si3N4, AlN, BN, aluminosilicates, C). The main sources of corrosion in combustion environment (proton, sodium ion) are discussed. A comparison is made with long-term corrosion at room-temperature. Examples of the different corrosion mechanisms observed for Nicalon NLM202 fibre glass-ceramic or ceramic (LAS, GAS, celsian, cordierite, Al2TiO5, mullite, Nasicon) matrix composites developed at ONERA are presented : ion exchange, grain boundary dissolution, fluxing, favourable and unfavourable fibre-matrix reaction, enhanced corrosion by prior fibre-matrix reaction.
引用
收藏
页码:833 / 844
页数:12
相关论文
共 46 条
[31]  
MAZEROLLES L, 1990, J PHYSIQUE S1, V51, P879
[32]  
MCCAULEY RA, 1990, CERAMICS T, V10
[33]  
MISRA AK, 1990, 4271 NASA
[34]   Microwave absorbent: Preparation, mechanical properties and rf-microwave conductivity of SiC (and/or mullite) fibre reinforced Nasicon matrix composites [J].
Mouchon, E ;
Colomban, P .
JOURNAL OF MATERIALS SCIENCE, 1996, 31 (02) :323-334
[35]   OXIDE CERAMIC-MATRIX OXIDE FIBER WOVEN FABRIC COMPOSITES EXHIBITING DISSIPATIVE FRACTURE-BEHAVIOR [J].
MOUCHON, E ;
COLOMBAN, P .
COMPOSITES, 1995, 26 (03) :175-182
[36]   HYDROGEN SUBSTITUTION IN LITHIUM-ALUMINOSILICATES [J].
MULLER, G ;
HOFFMANN, M ;
NEEFF, R .
JOURNAL OF MATERIALS SCIENCE, 1988, 23 (05) :1779-1785
[37]  
OLIVEIRA FAC, 1994, NATO ADV SCI INST SE, V267, P177
[38]   CORROSION OF CERAMIC-MATRIX COMPOSITES [J].
SCANU, T ;
COLOMBAN, P .
JOURNAL DE PHYSIQUE IV, 1993, 3 (C7) :1927-1930
[39]   ION-EXCHANGE AND HOT CORROSION OF CERAMIC COMPOSITES MATRICES - A VIBRATIONAL AND MICROSTRUCTURAL STUDY [J].
SCANU, T ;
GUGLIELMI, J ;
COLOMBAN, P .
SOLID STATE IONICS, 1994, 70 :109-120
[40]  
SCOTT V, 1993, HIGH TEMPERATURE CER, P691