Structure, hardness and thermal stability of TiAlN and nanolayered TiAlN/CrN multilayer films

被引:182
作者
Barshilia, HC
Prakash, MS
Jain, A
Rajam, KS
机构
[1] Natl Aerosp Labs, Surface Engn Div, Bangalore 560017, Karnataka, India
[2] Natl Aerosp Labs, Div Mat Sci, Bangalore 560017, Karnataka, India
关键词
TiAlN films; TiAlN/CrN multilayers; reactive DC magnetron sputtering; X-ray diffraction; nanoindentation; thermal stability;
D O I
10.1016/j.vacuum.2004.08.020
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TiAlN films were deposited on silicon (1 1 1) substrates from a TiAl target using a reactive DC magnetron sputtering process in Ar + N-2 plasma. Films were prepared at various nitrogen flow rates and TiAl target compositions. Similarly, CrN films were prepared from the reactive sputtering of Cr target. Subsequently, nanolayered TiAlN/CrN multilayer films were deposited at various modulation wavelengths (A). X-ray diffraction (XRD), energy dispersive X-ray analysis, nanoindentation and atomic force microscopy were used to characterize the films. The XRD confirmed the formation of superlattice structure at low modulation wavelengths. The maximum hardness of TiAlN/CrN multilayers was 3900 kg/mm(2), whereas TiAlN and CrN films exhibited maximum hardnesses of 3850 and 1000 kg/mm(2), respectively. Thermal stability of TiAlN and TiAlN/CrN multilayer films was studied by heating the films in air in the temperature range (T-A) of 500-900degreesC for 30 min. The XRD spectra revealed that TiAlN/CrN multilayers were stable up to 800degreesC and got oxidized substantially at 900degreesC. On the other hand, the TiAlN films were stable up to 700degreesC and got completely oxidized at 800degreesC. Nanoindentation measurements performed on the films after heat treatment showed that TiAlN retained a hardness of 2200 kg/mm(2) at T-A = 700degreesC and TiAlN/CrN multilayers retained hardness as high as 2600 kg/mm(2) upon annealing at 800degreesC. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:169 / 179
页数:11
相关论文
共 18 条
[1]   GRAIN-SIZE AND RECRYSTALLIZATION OF TIN, ZRN, NBN, AND CRN ALLOYED AND MULTILAYER FILMS [J].
ANDRIEVSKI, RA ;
ANISIMOVA, IA ;
ANISIMOV, VP ;
MAKAROV, VP ;
POPOVA, VP .
THIN SOLID FILMS, 1995, 261 (1-2) :83-86
[2]  
Barshilia HC, 2003, VACUUM, V72, P241, DOI 10.1016/j.vacuum.2003.008.003
[3]   MODEL OF SUPERLATTICE YIELD STRESS AND HARDNESS ENHANCEMENTS [J].
CHU, X ;
BARNETT, SA .
JOURNAL OF APPLIED PHYSICS, 1995, 77 (09) :4403-4411
[4]  
Cullity BD, 1978, ELEMENTS XRAY DIFFRA
[5]   GROWTH OF SINGLE-CRYSTAL TIN VN STRAINED-LAYER SUPERLATTICES WITH EXTREMELY HIGH MECHANICAL HARDNESS [J].
HELMERSSON, U ;
TODOROVA, S ;
BARNETT, SA ;
SUNDGREN, JE ;
MARKERT, LC ;
GREENE, JE .
JOURNAL OF APPLIED PHYSICS, 1987, 62 (02) :481-484
[6]   HIGH-TEMPERATURE OXIDATION OF ION-PLATED TIN AND TIALN FILMS [J].
ICHIMURA, H ;
KAWANA, A .
JOURNAL OF MATERIALS RESEARCH, 1993, 8 (05) :1093-1100
[7]   HIGH-TEMPERATURE OXIDATION OF ION-PLATED CRN FILMS [J].
ICHIMURA, H ;
KAWANA, A .
JOURNAL OF MATERIALS RESEARCH, 1994, 9 (01) :151-155
[8]   INDUSTRIAL DEPOSITION OF BINARY, TERNARY, AND QUATERNARY NITRIDES OF TITANIUM, ZIRCONIUM, AND ALUMINUM [J].
KNOTEK, O ;
MUNZ, WD ;
LEYENDECKER, T .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1987, 5 (04) :2173-2179
[9]   Localised oxidation defects in TiAlN/CrN superlattice structured hard coatings grown by cathodic arc/unbalanced magnetron deposition on various substrate materials [J].
Lembke, MI ;
Lewis, DB ;
Münz, WD .
SURFACE & COATINGS TECHNOLOGY, 2000, 125 (1-3) :263-268
[10]   ION INDUCED STRESS GENERATION IN ARC-EVAPORATED TIN FILMS [J].
LJUNGCRANTZ, H ;
HULTMAN, L ;
SUNDGREN, JE ;
KARLSSON, L .
JOURNAL OF APPLIED PHYSICS, 1995, 78 (02) :832-837