Ion irradiation of rare-earth- and yttrium-titanate-pyrochlores

被引:87
作者
Wang, SX
Wang, LM
Ewing, RC
Kutty, KVG
机构
[1] Univ Michigan, Dept Nucl Engn & Radiol Sci, Ann Arbor, MI 48109 USA
[2] Indira Gandhi Ctr Atom Res, Mat Chem Div, Kalpakkam 603102, Tamil Nadu, India
关键词
amorphization; pyrochlore; irradiation; nuclear waste form; TEM;
D O I
10.1016/S0168-583X(00)00030-6
中图分类号
TH7 [仪器、仪表];
学科分类号
0804 ; 080401 ; 081102 ;
摘要
Pyrochlore, A(1-2)B(2)O(6)(O,OH,F)(0-1), is an actinide-bearing phase in Synroc, a polyphase ceramic proposed for the immobilization of high level nuclear waste. Structural damage due to alpha-decay events can significantly affect the chemical and physical stability of the nuclear waste form. Pyrochlore can effectively incorporate a variety of actinides into its structure. Four titanate pyrochlores were synthesized with compositions of Gd(2)Ti(2)O(7), Sm(2)Ti(2)O(7), Eu(2)Ti(2)O(7) and Y(2)Ti(2)O(2). These samples were irradiated with 1 MeV Kr(+) in order to simulate alpha-decay damage and were observed by in situ electron microscopy. Irradiations were conducted from 25 K to 1023 K. At room temperature, Gd-, Sm- and Eu-pyrochlores amorphized at a dose of similar to 2 x 10(14) ions/cm(2) (similar to 0.5 dpa) and Y-pyrochlore amorphized at 4 x 10(14) ions/cm(2) (similar to 0.8 dpa). The amorphization dose became higher at elevated temperatures with different rates of increase for each composition. The critical temperatures for amorphization are similar to 1100 K for Gd-, Sm-, Eu-pyrochlore and similar to 780 K for Y-pyrochlore. The rare-earth-pyrochlores are more susceptible to amorphization and have higher critical temperatures than Y-pyrochlore, The difference in amorphization dose and critical temperature is attributed to the different cascade sizes caused by the different cation masses of the target. Based on a model of cascade quenching, the larger cascade is related to a lower amorphization dose and higher critical temperature. The irradiated materials were studied by electron diffraction and high-resolution electron microscopy. All the pyrochlores transformed to a fluorite substructure prior to the completion of amorphization of the observed regions. This transformation was caused by the disordering between cations and between oxygen and oxygen vacancies. The concurrence of cation disordering with amorphization suggests the partial recrystallization of the displacement cascades. Isolated cascade damage regions were observed by high-resolution electron microscopy, and the cation disordering was associated with the damaged regions. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:135 / 140
页数:6
相关论文
共 28 条
[1]   INSITU ION IRRADIATION IMPLANTATION STUDIES IN THE HVEM-TANDEM FACILITY AT ARGONNE-NATIONAL-LABORATORY [J].
ALLEN, CW ;
FUNK, LL ;
RYAN, EA ;
TAYLOR, A .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1989, 40-1 :553-556
[2]  
BEGG BD, 1999, IN PRESS WASTE MANAG
[3]   ALPHA-DECAY SELF-IRRADIATION DAMAGE IN PU-238-SUBSTITUTED ZIRCONOLITE [J].
CLINARD, FW ;
HOBBS, LW ;
LAND, CC ;
PETERSON, DE ;
ROHR, DL ;
ROOF, RB .
JOURNAL OF NUCLEAR MATERIALS, 1982, 105 (2-3) :248-256
[4]   The immobilization of high level radioactive wastes using ceramics and glasses [J].
Donald, IW ;
Metcalfe, BL ;
Taylor, RNJ .
JOURNAL OF MATERIALS SCIENCE, 1997, 32 (22) :5851-5887
[5]  
Ewing RC, 1996, NATO SCI S 1 DISARM, V4, P65
[6]   THE STRUCTURE OF APERIODIC, METAMICT (CA,TH)ZRTI2O7 (ZIRCONOLITE) - AN EXAFS STUDY OF THE ZR-SITES, TH-SITES AND U-SITES [J].
FARGES, F ;
EWING, RC ;
BROWN, GE .
JOURNAL OF MATERIALS RESEARCH, 1993, 8 (08) :1983-1995
[7]   A DEFECT MODEL FOR ION-INDUCED CRYSTALLIZATION AND AMORPHIZATION [J].
JACKSON, KA .
JOURNAL OF MATERIALS RESEARCH, 1988, 3 (06) :1218-1226
[8]   Activation energies for light ions in ion beam induced epitaxial crystallization [J].
Kinomura, A ;
Chayahara, A ;
Tsubouchi, N ;
Horino, Y ;
Williams, JS .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1999, 148 (1-4) :370-374
[9]   Ion transport studies on vacuum deposited PbSnI4 thin films [J].
Kuku, TA .
THIN SOLID FILMS, 1999, 340 (1-2) :292-296
[10]   Alpha-recoil damage in zirconolite (CaZrTi2O7) [J].
Lumpkin, G. R. ;
Ewing, R. C. ;
Chakoumakos, B. C. ;
Greegor, R. B. ;
Lytle, F. W. ;
Foltyn, E. M. ;
Clinard, F. W., Jr. ;
Boatner, L. A. ;
Abraham, M. M. .
JOURNAL OF MATERIALS RESEARCH, 1986, 1 (04) :564-576