STRENGTH RETENTION OF SELF-REINFORCED POLY-L-LACTIDE SCREWS AND PLATES - AN INVIVO AND INVITRO STUDY

被引:61
作者
SUURONEN, R
POHJONEN, T
TAURIO, R
TORMALA, P
WESSMAN, L
RONKKO, K
VAINIONPAA, S
机构
[1] TAMPERE UNIV,INST PLAST TECHNOL,BIOMAT LAB,SF-33101 TAMPERE,FINLAND
[2] COLL VET MED,DEPT SURG,SF-00580 HELSINKI,FINLAND
[3] HELSINKI UNIV,CENT HOSP,DEPT ORTHOPAED & TRAUMATOL,SF-00260 HELSINKI,FINLAND
关键词
D O I
10.1007/BF00701239
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Self-reinforced poly-L-lactide (SR-PLLA) screws and multilayer plates were studied for their initial mechanical shear and/or tensile strength and strength retention in vivo and in vitro up to 48 weeks. The plates were studied in vitro up to 68 weeks. The loss of strength was faster in vivo than in vitro. The screws retained more than half of their initial shear strength up to 12 weeks in vivo and over 24 weeks in vitro. By 48 weeks they had lost nearly all of their mechanical strength in both groups. The plates retained over 54% of their initial tensile and 71% of shear strength up to 24 weeks in vivo. The shear strength did not particularly diminish up to 52 weeks of follow-up in vitro whereas the tensile strength was slightly decreased after 36 weeks. After this follow-up time the loss of strength was more rapid and by 68 weeks the shear strength had decreased to 17% and the tensile strength to 0%.
引用
收藏
页码:426 / 431
页数:6
相关论文
共 43 条
[12]  
CUTRIGHT DE, 1971, J ORAL SURG, V29, P393
[13]  
CUTRIGHT DE, 1972, ORAL SURG ORAL MED O, V33, P28, DOI 10.1016/0030-4220(72)90204-6
[14]   TISSUE REACTION TO BIODEGRADABLE POLYLACTIC ACID SUTURE [J].
CUTRIGHT, DE ;
HUNSUCK, EE .
ORAL SURGERY ORAL MEDICINE ORAL PATHOLOGY ORAL RADIOLOGY AND ENDODONTICS, 1971, 31 (01) :134-&
[15]  
CUTRIGHT DE, 1974, ORAL SURG, V37, P143
[16]   INVESTIGATION OF STRUCTURE OF SOLUTION GROWN CRYSTALS OF LACTIDE COPOLYMERS BY MEANS OF CHEMICAL-REACTIONS [J].
FISCHER, EW ;
STERZEL, HJ ;
WEGNER, G .
KOLLOID-ZEITSCHRIFT AND ZEITSCHRIFT FUR POLYMERE, 1973, 251 (11) :980-990
[17]  
Gerlach KL, 1987, BIOMATERIALS CLIN AP, P439
[18]  
GERLACH KL, 1987, BIOMATERIALS CLIN AP, P459
[19]  
GETTER L, 1972, J ORAL SURG, V30, P344
[20]   FRACTURE FIXATION WITH BIODEGRADABLE RODS - 41 CASES OF SEVERE ANKLE FRACTURES [J].
HIRVENSALO, E .
ACTA ORTHOPAEDICA SCANDINAVICA, 1989, 60 (05) :601-606