Cyclic fatigue growth rates in R-curve ceramics have been observed to depend very strongly on the maximum applied stress intensity, K-max, and only weakly on the stress intensity range, Delta K. This behavior is rationalized through measurement of crack wake shielding characteristics as a function of these fatigue parameters in a gas-pressure-sintered silicon nitride. In particular, evidence for a mechanical equilibrium between shielding accumulation by crack growth and shielding degradation by frictional wear of sliding interfaces is found for steady-state cyclic fatigue. This equilibrium gives rise to a rate law for cyclic fatigue. The data suggest that the accumulation process is the origin of the strong K-max dependence, and that the degradation process is the origin of the weak Delta K dependence, These features are shown to be related to the ''cyclic'' R-curve and to the cyclic crack opening displacement, respectively.
引用
收藏
页码:513 / 520
页数:8
相关论文
共 45 条
[31]   THE MECHANICS OF MATRIX CRACKING IN BRITTLE-MATRIX FIBER COMPOSITES [J].
MARSHALL, DB ;
COX, BN ;
EVANS, AG .
ACTA METALLURGICA, 1985, 33 (11) :2013-2021
[32]  
OJAYI OO, 1989, WEAR MATER, V1, P349
[33]   SUBCRITICAL CRACK-GROWTH IN SINTERED SILICON-NITRIDE EXHIBITING A RISING R-CURVE [J].
OKADA, A ;
HIROSAKI, N ;
YOSHIMURA, M .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (07) :2095-2096
[34]   IMPROVED FLAW TOLERANCE IN ALUMINA CONTAINING 1-VOL-PERCENT ANORTHITE VIA CRYSTALLIZATION OF THE INTERGRANULAR GLASS [J].
PADTURE, NP ;
CHAN, HM .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (07) :1870-1875
[35]   MATRIX CRACKING IN UNIDIRECTIONAL CERAMIC MATRIX COMPOSITES UNDER QUASI-STATIC AND CYCLIC LOADING [J].
PRYCE, AW ;
SMITH, PA .
ACTA METALLURGICA ET MATERIALIA, 1993, 41 (04) :1269-1281
[36]  
REICHL A, 1988, J AM CERAM SOC, V71, pC299, DOI 10.1111/j.1151-2916.1988.tb05908.x
[37]   INSITU MEASUREMENTS OF BRIDGED CRACK INTERFACES IN THE SCANNING ELECTRON-MICROSCOPE [J].
RODEL, J ;
KELLY, JF ;
LAWN, BR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (11) :3313-3318
[38]   FRACTURE-TOUGHNESS OF SI3N4 MEASURED WITH SHORT BAR CHEVRON-NOTCHED SPECIMENS [J].
SALEM, JA ;
SHANNON, JL .
JOURNAL OF MATERIALS SCIENCE, 1987, 22 (01) :321-324
[39]   R-CURVE BEHAVIOR OF LONG CRACKS IN ALUMINA [J].
STEINBRECH, RW ;
REICHL, A ;
SCHAARWACHTER, W .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (07) :2009-2015
[40]   CRACK-INTERFACE GRAIN BRIDGING AS A FRACTURE-RESISTANCE MECHANISM IN CERAMICS .1. EXPERIMENTAL-STUDY ON ALUMINA [J].
SWANSON, PL ;
FAIRBANKS, CJ ;
LAWN, BR ;
MAI, YW ;
HOCKEY, BJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1987, 70 (04) :279-289