HIGH-TEMPERATURE ENVIRONMENTAL STRENGTH DEGRADATION OF A HOT-PRESSED SILICON-NITRIDE - AN EXPERIMENTAL TEST

被引:15
作者
CLARKE, DR [1 ]
机构
[1] ROCKWELL INT CORP,CTR SCI,STRUCT CERAM GRP,THOUSAND OAKS,CA 91360
关键词
D O I
10.1111/j.1151-2916.1983.tb09995.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
引用
收藏
页码:156 / 158
页数:3
相关论文
共 17 条
[11]   EVIDENCE FOR CAVITATION CRACK GROWTH IN SI3N4 [J].
LANGE, FF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1979, 62 (3-4) :222-223
[12]   EUTECTIC STUDIES IN THE SYSTEM SI3N4-SI2N2O-MG2SIO4 [J].
LANGE, FF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1979, 62 (11-1) :617-619
[13]   HIGH-TEMPERATURE STRENGTH BEHAVIOR OF HOT-PRESSED SI3N4 - EVIDENCE FOR SUBCRITICAL CRACK GROWTH [J].
LANGE, FF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1974, 57 (02) :84-87
[14]   IMPURITY PHASES IN HOT-PRESSED SI3N4 [J].
LOU, LKV ;
MITCHELL, TE ;
HEUER, AH .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1978, 61 (9-10) :392-396
[15]   THERMODYNAMICS AND KINETICS OF OXIDATION OF HOT-PRESSED SILICON-NITRIDE [J].
SINGHAL, SC .
JOURNAL OF MATERIALS SCIENCE, 1976, 11 (03) :500-509
[16]   MOLTEN-SALT CORROSION OF SIC AND SI-3N-4 CERAMICS [J].
TRESSLER, RE ;
MEISER, MD ;
YONUSHONIS, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (5-6) :278-279
[17]   OXIDATION OF SI3N4 IN RANGE 1300DEGREESC TO 1500DEGREESC [J].
TRIPP, WC ;
GRAHAM, HC .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (9-10) :399-403