This paper reports on the thermal stability of ZrN-Ni and CrN-Ni nanocomposite coatings with a nickel content between approximately 0.5 and 8 at.%, which were prepared by DC reactive magnetron sputtering at a substrate temperature of 300 and 200 degreesC, respectively, and a negative bias between -30 and -200 V for ZrN-Ni and -200 V for CrN-Ni. The films were characterised by X-ray diffraction (XRD), Vickers hardness measurements and X-ray photoelectron spectroscopy (XPS). Upon isochronal annealing in a forming gas (90 vol.% N-2, 10 vol.% H-2) between 400 and 650 degreesC for 30 min, the hardness and lattice parameter of crystal planes parallel to the substrate decreased, indicating that the hardness enhancement is due to a high biaxial compressive stress in the coatings. No hardness enhancement could be attributed to the formation of a nanocomposite structure. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:280 / 285
页数:6
相关论文
共 34 条