Characteristics of the thermal oxidation of heavily boron-doped polycrystalline silicon thin films

被引:10
作者
Boukezzata, M [1 ]
BielleDaspet, D [1 ]
Sarrabayrouse, G [1 ]
Mansour, F [1 ]
机构
[1] CNRS,LAAS,F-31077 TOULOUSE,FRANCE
关键词
oxidation; chemical vapour deposition; boron; silicon; ion implantation;
D O I
10.1016/0040-6090(95)08172-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Dry oxidation kinetics were compared for 2 x 10(20) cm(-3) boron-implanted and in-situ doped films deposited at temperatures ranging between 520 and 620 degrees C. The characteristics of the thermal oxidation of these films have been studied over the oxidation temperature range of 750 to 1050 degrees C and for durations of 10 min to 26 h. High values of both the surface oxidation rate k(s) and the oxide diffusion coefficient D are evidenced as typical of the in-situ doped films. In addition to the well-known effect that heavy doping increases the rate of oxidation similar to what is observed in single-crystal silicon, it is also shown specially, for the in-situ boron-doped films compared with 2 x 10(20) cm(-3) in-situ phosphorus-doped ones, that the greatest oxidation rate is observed at high oxidation temperatures (T-ox > 1000 degrees C). This enhancement is related to some specific factors of these materials, such as grain boundary structures, defects, texture and electrical properties related to the segregation and supersaturation phenomenon which occur at these levels of doping.
引用
收藏
页码:145 / 154
页数:10
相关论文
共 21 条
  • [1] INTERFACE REACTION OF B2O3-SI SYSTEM AND BORON DIFFUSION INTO SILICON
    ARAI, E
    TERUNUMA, Y
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1973, 120 (07) : 980 - 987
  • [2] ARMIGLIATO A, 1977, J ELECTROCHEM SOC, P638
  • [3] BAUDET J, 1988, 88227 LAAS CNRS
  • [4] MICROSTRUCTURE OF BORON-DOPED SILICON LAYERS PREPARED BY LOW-PRESSURE CHEMICAL VAPOR-DEPOSITION
    BIELLEDASPET, D
    MANSOURBAHLOUI, F
    MARTINEZ, A
    PIERAGGI, B
    DAVID, MJ
    DEMAUDUIT, B
    OUSTRY, A
    CARLES, R
    LANDA, G
    AJUSTRON, F
    MAZEL, A
    RIBOULET, P
    [J]. THIN SOLID FILMS, 1987, 150 (01) : 69 - 82
  • [5] STRUCTURAL AND TECHNOLOGICAL PROPERTIES OF HEAVILY INSITU PHOSPHORUS-DOPED LOW-PRESSURE CHEMICALLY VAPOR-DEPOSITED SILICON FILMS
    BIELLEDASPET, D
    MERCADERE, L
    BOUKEZZATA, M
    PIERAGGI, B
    DEMAUDUIT, B
    [J]. THIN SOLID FILMS, 1989, 175 : 43 - 48
  • [6] MATERIAL AND ELECTRONIC-PROPERTIES OF BORON-DOPED SILICON FILMS DEPOSITED FROM SIH4-BCL3-N2 MIXTURES IN AN INDUSTRIAL LOW-PRESSURE CHEMICAL VAPOR-DEPOSITION FURNACE
    BIELLEDASPET, D
    SCHEID, E
    AZZARO, C
    DEMAUDUIT, B
    PIERAGGI, B
    [J]. THIN SOLID FILMS, 1991, 204 (01) : 33 - 48
  • [7] Boukezzata M., 1988, THESIS U P SABATIER
  • [8] Deal B. E., 1965, J APPL PHYS, V132, P2815
  • [9] GROVE AS, 1967, PHYS TECHNOL S, P27
  • [10] PARALLEL OXIDATION MECHANISM FOR SI OXIDATION IN DRY O2
    HAN, CJ
    HELMS, CR
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1987, 134 (05) : 1297 - 1302