Electrochemical characterization of Fe-Ni-P alloy electrodeposition

被引:50
作者
Sridharan, K
Sheppard, K
机构
[1] Dept. of Mat. Sci. and Engineering, Stevens Institute of Technology, Hoboken
关键词
alloy; amorphous; anomalous; hydrogen; iron; nickel; phosphorus; plating;
D O I
10.1023/A:1018475718629
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
In this study we have investigated the electrodeposition of amorphous iron-nickel-phosphorus alloys from a sulfate electrolyte. Fe-Ni alloys are known to exhibit an 'anomalous' type of plating behaviour in which deposition of the less noble metal is favoured. We have found that the codeposition of phosphorus from hypophosphite in the electrolyte led to a reversal to a 'normal' behaviour. This reversal was due both to the suppression of iron and enhancement of nickel partial currents. The overall deposition process is dominated by the hydrogen evolution reaction. This is exacerbated by the low pH needed to codeposit sufficient phosphorus to achieve an amorphous structure.
引用
收藏
页码:1198 / 1206
页数:9
相关论文
共 38 条
[21]   THE BANDED STRUCTURE OF NI-P ELECTRODEPOSITS [J].
NEE, CC ;
WEIL, R .
SURFACE TECHNOLOGY, 1985, 25 (01) :7-15
[22]   STRUCTURE OF AMORPHOUS FE-CR-P ALLOYS PREPARED BY ELECTRODEPOSITION [J].
NG, PK ;
MITCHELL, TE ;
LOCCI, IE ;
RUIZ, AA .
JOURNAL OF MATERIALS RESEARCH, 1989, 4 (02) :300-308
[23]  
Ogburn F., 1973, Plating, V60, P1043
[24]   ELECTRODEPOSITION OF HIGH MO CONTENT NI-MO ALLOYS UNDER FORCED-CONVECTION [J].
PODLAHA, EJ ;
MATLOSZ, M ;
LANDOLT, D .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (10) :L149-L151
[25]   GALVANOSTATIC PULSE AND PULSE REVERSE PLATING OF NICKEL-IRON ALLOYS FROM ELECTROLYTES CONTAINING ORGANIC-COMPOUNDS ON A ROTATING-DISK ELECTRODE [J].
POPOV, BN ;
YIN, KM ;
WHITE, RE .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (05) :1321-1330
[26]  
RATZKER M, 1986, PLAT SURF FINISH, V73, P74
[27]   CHEMICAL NICKEL-IRON FILMS [J].
SCHMECKE.AF .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1966, 113 (08) :778-&
[28]  
Sridharan K., 1994, T IMF, V72, p153?158, DOI [10.1080/00202967.1994.11871044, DOI 10.1080/00202967.1994.11871044]
[29]  
SRIDHARAN K, IN PRESS J MAT PROCE
[30]  
SRIMATHI SN, 1982, SURF TECHNOL, V16, P272