Mechanical properties of single electrospun drug-encapsulated nanofibres

被引:160
作者
Chew, Sing Yian
Hufnagel, Todd C.
Lim, Chwee Teck
Leong, Kam W. [1 ]
机构
[1] Duke Univ, Dept Biomed Engn, Durham, NC 27708 USA
[2] Johns Hopkins Univ, Dept Mat Sci & Engn, Baltimore, MD 21218 USA
[3] Natl Univ Singapore, Div Bioengn, Singapore 117576, Singapore
[4] Natl Univ Singapore, Dept Mech Engn, Singapore 117576, Singapore
关键词
D O I
10.1088/0957-4484/17/15/045
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The mechanical and structural properties of a surface play an important role in determining the morphology of attached cells, and ultimately their cellular functions. As such, mechanical and structural integrity are important design parameters for a tissue scaffold. Electrospun fibrous meshes are widely used in tissue engineering. When in contact with electrospun scaffolds, cells see the individual micro- or nanofibres as their immediate microenvironment. In this study, tensile testing of single electrospun nanofibres composed of poly(epsilon-caprolactone) (PCL), and its copolymer, poly(caprolactone-co-ethyl ethylene phosphate) (PCLEEP), revealed a size effect in the Young's modulus, E, and tensile strength, sigma(T). Both strength and stiffness increase as the fibre diameter decreases from bulk (similar to 5 mu m) into the nanometre region (200-300 nm). In particular, E and sigma(T) of individual PCL nanofibres were at least two-fold and an order of magnitude higher than that of PCL film, respectively. PCL films were observed to have more pronounced crystallographic texture than the nanofibres; however no difference in crystalline fraction, perfection, or texture was detected among the various fibres. When drugs were encapsulated into single PCLEEP fibres, mechanical properties were enhanced with 1-20 wt% of loaded retinoic acid, but weakened by 10-20 wt% of encapsulated bovine serum albumin. This understanding of the effect of size and drug and protein encapsulation on the mechanical properties of electrospun fibres may help in the optimization of tissue scaffold design that combines biochemical and biomechanical cues for tissue regeneration.
引用
收藏
页码:3880 / 3891
页数:12
相关论文
共 55 条
[41]   Mechanical properties and cellular proliferation of electrospun collagen type II [J].
Shields, KJ ;
Beckman, MJ ;
Bowlin, GL ;
Wayne, JS .
TISSUE ENGINEERING, 2004, 10 (9-10) :1510-1517
[42]   Arterial smooth muscle cell proliferation on a novel biomimicking, biodegradable vascular graft scaffold [J].
Stitzel, JD ;
Pawlowski, KJ ;
Wnek, GE ;
Simpson, DG ;
Bowlin, GL .
JOURNAL OF BIOMATERIALS APPLICATIONS, 2001, 16 (01) :22-33
[43]   Mechanical characterization of nanofibers - A review [J].
Tan, E. P. S. ;
Lim, C. T. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2006, 66 (09) :1102-1111
[44]   Tensile test of a single nanofiber using an atomic force microscope tip [J].
Tan, EPS ;
Goh, CN ;
Sow, CH ;
Lim, CT .
APPLIED PHYSICS LETTERS, 2005, 86 (07) :1-3
[45]   Tensile testing of a single ultrafine polymeric fiber [J].
Tan, EPS ;
Ng, SY ;
Lim, CT .
BIOMATERIALS, 2005, 26 (13) :1453-1456
[46]   Physical properties of a single polymeric nanofiber [J].
Tan, EPS ;
Lim, CT .
APPLIED PHYSICS LETTERS, 2004, 84 (09) :1603-1605
[47]   Tuning compliance of nanoscale polyelectrolyte multilayers to modulate cell adhesion [J].
Thompson, MT ;
Berg, MC ;
Tobias, IS ;
Rubner, MF ;
Van Vliet, KJ .
BIOMATERIALS, 2005, 26 (34) :6836-6845
[48]   Substrate flexibility regulates growth and apoptosis of normal but not transformed cells [J].
Wang, HB ;
Dembo, M ;
Wang, YL .
AMERICAN JOURNAL OF PHYSIOLOGY-CELL PHYSIOLOGY, 2000, 279 (05) :C1345-C1350
[49]  
Wen J, 1998, POLYM INT, V47, P503, DOI 10.1002/(SICI)1097-0126(199812)47:4<503::AID-PI90>3.3.CO
[50]  
2-E