Potentiometry and repair of electrically stressed nanowires using atomic force microscopy

被引:42
作者
Hersam, MC [1 ]
Hoole, ACF [1 ]
O'Shea, SJ [1 ]
Welland, ME [1 ]
机构
[1] Univ Cambridge, Dept Engn, Cambridge CB2 1PZ, England
关键词
D O I
10.1063/1.120872
中图分类号
O59 [应用物理学];
学科分类号
摘要
Using an atomic force microscope equipped with a conducting diamond tip, the surface potential on a current carrying gold nanowire was measured with microvolt potential sensitivity and nanometer spatial resolution. Potentiometry images illustrate the stages of failure of nanowires subjected to current stressing. During this failure process, a discontinuity in the potential gradient and an enhanced resistance region were observed at the failure site until a complete fracture was formed. By increasing the repulsive force and accurately positioning the tip, gold could be manipulated into the nanoscale fracture so that the electrical conductivity of the nanowire was regained. (C) 1998 American Institute of Physics.
引用
收藏
页码:915 / 917
页数:3
相关论文
共 13 条
  • [1] BROERS AN, 1989, MICROELECTRON ENG, V9, P18
  • [2] Scanning probe microscopy for testing ultrafast electronic devices
    Hou, AS
    Nechay, BA
    Ho, F
    Bloom, DM
    [J]. OPTICAL AND QUANTUM ELECTRONICS, 1996, 28 (07) : 819 - 841
  • [3] HUMMEL RE, 1994, INT MATER REV, V39, P97, DOI 10.1179/095066094790326194
  • [4] Johnson K. L., 1987, CONTACT MECH
  • [5] Vacuum compatible high-sensitive Kelvin probe force microscopy
    Kikukawa, A
    Hosaka, S
    Imura, R
    [J]. REVIEW OF SCIENTIFIC INSTRUMENTS, 1996, 67 (04) : 1463 - 1467
  • [6] HIGH-RESOLUTION CAPACITANCE MEASUREMENT AND POTENTIOMETRY BY FORCE MICROSCOPY
    MARTIN, Y
    ABRAHAM, DW
    WICKRAMASINGHE, HK
    [J]. APPLIED PHYSICS LETTERS, 1988, 52 (13) : 1103 - 1105
  • [7] The metallurgical control of electromigration failure in narrow conducting lines
    Morris, JW
    Kim, CU
    Kang, SH
    [J]. JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1996, 48 (05): : 43 - 46
  • [8] SCANNING TUNNELING POTENTIOMETRY
    MURALT, P
    POHL, DW
    [J]. APPLIED PHYSICS LETTERS, 1986, 48 (08) : 514 - 516
  • [9] Chemical vapor deposition diamond for tips in nanoprobe experiments
    Niedermann, P
    Hanni, W
    Blanc, N
    Christoph, R
    Burger, J
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 1996, 14 (03): : 1233 - 1236
  • [10] KELVIN PROBE FORCE MICROSCOPY
    NONNENMACHER, M
    OBOYLE, MP
    WICKRAMASINGHE, HK
    [J]. APPLIED PHYSICS LETTERS, 1991, 58 (25) : 2921 - 2923