TRANSPORT AND PHOTOLUMINESCENCE OF HYDROGENATED AMORPHOUS SILICON-CARBON ALLOYS

被引:57
作者
CHU, V
CONDE, JP
JAREGO, J
BROGUEIRA, P
RODRIGUEZ, J
BARRADAS, N
SOARES, JC
机构
[1] INST SUPER TECN, DEPT PHYS, P-1096 LISBON, PORTUGAL
[2] UNIV LISBON, CTR FIS NUCL, P-1699 LISBON, PORTUGAL
[3] UNIV NACL INGN LIMA, FAC CIENCIAS, DEPT FIS, LIMA, PERU
关键词
D O I
10.1063/1.360005
中图分类号
O59 [应用物理学];
学科分类号
摘要
The optoelectronic properties of hydrogenated amorphous silicon-carbon alloys (a-SiC:H) are studied over the entire compositional range of carbon content. The films are prepared using radio-frequency glow discharge and optimization was made with respect to deposition power and pressure, hydrogen dilution, and methane (or ethylene) -to-silane gas phase ratio. Regardless of the deposition conditions and source gases used, the optical, structural, and transport properties of the a-SiC:H alloys followed simple universal dependencies related to changes in the density of states associated with their structural disorder. The Urbach tail energy E(u) and the B factor of the Tauc plot correlate with E(04) (defined as the energy at which the absorption coefficient is equal to 10(4) cm(-1)) taken from photothermal deflection spectroscopy measurements. Up to E(04)(pds)approximate to 2.6 eV, E(u) increases monotonically from 50 up to approximate to 200 meV, while the B factor decreases from approximate to 800 down to approximate to 200 cm(-1/2)eV(-1/2). Above E(04)(pds)approximate to 2.6 eV, both E(u) and B remain approximately constant. The photoconductivity decreases exponentially with E(04)(pds) and is below 10(-10) Ohm(-1) cm(-1) for E(04)(pds)greater than or equal to 2.6 eV. Room-temperature photoluminescence is observed when E(04)(pds)greater than or equal to 2.6 eV. The photoluminescence peak position lies an average of 0.6 eV below the value of E(04)(pds) and increases linearly with decreasing value of the B factor of the Tauc plot. (C) 1995 American Institute of Physics.
引用
收藏
页码:3164 / 3173
页数:10
相关论文
共 34 条
[1]   PHYSICS OF AMORPHOUS-SILICON CARBON ALLOYS [J].
BULLOT, J ;
SCHMIDT, MP .
PHYSICA STATUS SOLIDI B-BASIC SOLID STATE PHYSICS, 1987, 143 (02) :345-418
[2]   DIFFERENCES IN PHYSICAL-PROPERTIES OF HYDROGENATED AND FLUORINATED AMORPHOUS-SILICON CARBIDE PREPARED BY REACTIVE SPUTTERING [J].
DEMICHELIS, F ;
PIRRI, CF ;
TRESSO, E ;
STAPINSKI, T .
JOURNAL OF APPLIED PHYSICS, 1992, 71 (11) :5641-5645
[3]   PHOTO-LUMINESCENCE IN AMORPHOUS SYSTEM SIXC1-X [J].
ENGEMANN, D ;
FISCHER, R ;
KNECHT, J .
APPLIED PHYSICS LETTERS, 1978, 32 (09) :567-568
[4]  
GALLONI R, 1994, MATER RES SOC SYMP P, V336, P517, DOI 10.1557/PROC-336-517
[5]   OPTICAL AND TRIBOLOGICAL PROPERTIES OF HEAT-TREATED DIAMOND-LIKE CARBON [J].
GRILL, A ;
PATEL, V ;
MEYERSON, BS .
JOURNAL OF MATERIALS RESEARCH, 1990, 5 (11) :2531-2537
[6]   STRUCTURAL, COMPOSITIONAL AND OPTICAL-PROPERTIES OF HYDROGENATED AMORPHOUS-SILICON CARBON ALLOYS [J].
HERREMANS, H ;
GREVENDONK, W ;
VANSWAAIJ, RACMM ;
VANSARK, WGJHM ;
BERNTSEN, AJM ;
BIK, WMA ;
BEZEMER, J .
PHILOSOPHICAL MAGAZINE B-PHYSICS OF CONDENSED MATTER STATISTICAL MECHANICS ELECTRONIC OPTICAL AND MAGNETIC PROPERTIES, 1992, 66 (06) :787-800
[7]   DIRECT MEASUREMENT OF GAP-STATE ABSORPTION IN HYDROGENATED AMORPHOUS-SILICON BY PHOTOTHERMAL DEFLECTION SPECTROSCOPY [J].
JACKSON, WB ;
AMER, NM .
PHYSICAL REVIEW B, 1982, 25 (08) :5559-5562
[8]   CHEMICAL BONDING STATES IN THE AMORPHOUS SIXC1-X-H SYSTEM STUDIED BY X-RAY PHOTOEMISSION SPECTROSCOPY AND INFRARED-ABSORPTION SPECTRA [J].
KATAYAMA, Y ;
USAMI, K ;
SHIMADA, T .
PHILOSOPHICAL MAGAZINE B-PHYSICS OF CONDENSED MATTER STATISTICAL MECHANICS ELECTRONIC OPTICAL AND MAGNETIC PROPERTIES, 1981, 43 (02) :283-294
[9]   A STUDY OF VISIBLE-LIGHT INJECTION-ELECTROLUMINESCENCE IN A-SIC/P-I-N DIODE [J].
KRUANGAM, D ;
ENDO, T ;
WEI, GP ;
NONOMURA, S ;
OKAMOTO, H ;
HAMAKAWA, Y .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1985, 77-8 :1429-1432
[10]  
KUWANO Y, 1982, 16TH P IEEE PHOT SPE, P1338