Physical and predictive models of ultra thin oxide reliability in CMOS devices and circuits

被引:82
作者
Stathis, JH [1 ]
机构
[1] IBM Corp, Div Res, Thomas J Watson Res Ctr, Yorktown Hts, NY 10598 USA
来源
39TH ANNUAL PROCEEDINGS: INTERNATIONAL RELIABILITY PHYSICS SYMPOSIUM 2001 | 2001年
关键词
D O I
10.1109/RELPHY.2001.922893
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The microelectronics industry owes its considerable success largely to the existence of the thermal oxide of silicon. However, recently there is concern that the reliability of ultra-thin dielectrics will limit further scaling to slightly thinner than 2nm. This paper will review the physics and statistics of dielectric wearout and breakdown in ultra thin SiO2-based gate dielectrics. Electrons or holes tunneling through the gate oxide generate defects until a critical density is reached and the oxide breaks down. The critical defect density is explained by the formation of a percolation path of defects across the oxide. Only < 1% of the these paths ultimately lead to destructive breakdown, and the microscopic nature of these defects is not known. The rate of defect generation decreases approximately exponentially with supply voltage, below a threshold voltage of about 5 V for hot electron induced hydrogen release. However, the tunnel current also increases exponentially with decreasing oxide thickness, leading to a decreasing time-to-breakdown and a diminishing margin for reliability as device dimensions are scaled. Estimating the reliability of the dielectric requires an extrapolation from the measurement conditions (e.g. higher voltage) to operation conditions. Because of the diminished reliability margin, it has become imperative to try to reduce the error in this extrapolation. Long term(>1 year) stress experiments are now being used to measure the wearout and breakdown of ultra thin (a nm) dielectric films as close as possible to operating conditions. These measurements have revealed the details of the voltage dependence of the defect generation rate and critical defect density, allowing better modeling of the voltage dependence of the time-to-breakdown. Such measurements are used to guide the technology development prior to the manufacturing stage. We then discuss the nature of the electrical conduction through a breakdown spot, and the effect of the oxide breakdown on device and circuit performance. In some cases an oxide breakdown does not lead to immediate circuit failure, so more research is needed in order to develop a quantitative methodology for predicting the reliability of circuits.
引用
收藏
页码:132 / 149
页数:18
相关论文
共 198 条
  • [111] Soft breakdown in ultrathin SiO2 layers:: The conduction problem from a new point of view
    Miranda, E
    Suñé, J
    Rodríguez, R
    Nafría, M
    Martín, F
    Aymerich, X
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 1999, 38 (4B): : 2223 - 2226
  • [112] Detection and fitting of the soft breakdown failure mode in MOS structures
    Miranda, E
    Suñé, J
    Rodríguez, R
    Nafría, M
    Aymerich, X
    [J]. SOLID-STATE ELECTRONICS, 1999, 43 (09) : 1801 - 1805
  • [113] A study of the effect of deuterium on stress-induced leakage current
    Mitani, Y
    Satake, H
    Ito, H
    Toriumi, A
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 2000, 39 (6B): : L564 - L566
  • [114] Highly reliable gate oxide under Fowler-Nordheim electron injection by deuterium pyrogenic oxidation and deuterated poly-Si deposition
    Mitani, Y
    Satake, H
    Itoh, H
    Toriumi, A
    [J]. INTERNATIONAL ELECTRON DEVICES MEETING 2000, TECHNICAL DIGEST, 2000, : 343 - 346
  • [115] Nelson WB., 1990, ACCELERATED TESTING
  • [116] Nicollian P. E., 2000, 2000 IEEE International Reliability Physics Symposium Proceedings. 38th Annual (Cat. No.00CH37059), P7, DOI 10.1109/RELPHY.2000.843884
  • [117] Extending the reliability scaling limit of SiO2 through plasma nitridation
    Nicollian, PE
    Baldwin, GC
    Eason, KN
    Grider, DT
    Hattangady, SV
    Hu, JC
    Hunter, WR
    Rodder, M
    Rotondaro, ALP
    [J]. INTERNATIONAL ELECTRON DEVICES MEETING 2000, TECHNICAL DIGEST, 2000, : 545 - 548
  • [118] FRACTAL DIMENSION OF DIELECTRIC-BREAKDOWN
    NIEMEYER, L
    PIETRONERO, L
    WIESMANN, HJ
    [J]. PHYSICAL REVIEW LETTERS, 1984, 52 (12) : 1033 - 1036
  • [119] A fast and simple methodology for lifetime prediction of ultra-thin oxides
    Nigam, T
    Degraeve, R
    Groeseneken, G
    Heyns, MM
    Maes, HE
    [J]. 1999 IEEE INTERNATIONAL RELIABILITY PHYSICS SYMPOSIUM PROCEEDINGS - 37TH ANNUAL, 1999, : 381 - 388
  • [120] TRAP GENERATION AND OCCUPATION DYNAMICS IN SIO2 UNDER CHARGE INJECTION STRESS
    NISSANCOHEN, Y
    SHAPPIR, J
    FROHMANBENTCHKOWSKY, D
    [J]. JOURNAL OF APPLIED PHYSICS, 1986, 60 (06) : 2024 - 2035