Sol-gel modified poly(dimethylsiloxane) microfluidic devices with high electroosmotic Mobilities and hydrophilic channel wall characteristics

被引:182
作者
Roman, GT [1 ]
Hlaus, T [1 ]
Bass, KJ [1 ]
Seelhammer, TG [1 ]
Culbertson, CT [1 ]
机构
[1] Kansas State Univ, Manhattan, KS 66506 USA
关键词
D O I
10.1021/ac048811z
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
Using a sol-gel method, we have fabricated poly(dimethylsiloxane) (PDMS) microchips with SiO2 particles homogeneously distributed within the PDMS polymer matrix. These particles are similar to 10 nm in diameter. To fabricate such devices, PDMS (Sylgard 184) was cast against SU-8 molds. After curing, the chips were carefully removed from the mold and sealed against flat, cured pieces of PDMS to form enclosed channel manifolds. These chips were then solvated in tetraethyl orthosilicate (TEOS), causing them to expand. Subsequently, the chips were placed in an aqueous solution containing 2.8% ethylamine and heated to form nanometer-sized SiO2 particles within the cross-linked PDMS polymer. The water contact angle for the PDMS-SiO2 chips was similar to 90.2degrees compared to a water contact angle for Sylgard 184 of similar to 108.5degrees. More importantly, the SiO2 modified PDMS chips showed no rhodamine B absorption after 4 h, indicating a substantially more hydrophilic and nonabsorptive surface than native PDMS. Initial electroosmotic mobilities (EOM) of (8.3 +/- 0.2) x 10(-4) CM2/(V.S) (RSD = 2.6% (RSD is relative standard deviation); n = 10) were measured. Ibis value was approximately twice that of native Sylgard 184 PDMS chips (4.21 +/- 0.09) x 10(-4) CM2/(V.S) (RSD = 2.2%; n =10) and 55% greater than glass chips (5.3 +/- 0.4) x 10(-4) CM2/(V.S) (RSD = 7.7%; n 5). After 60 days of dry storage, the EOM was (7.6 +/- 0.3) x 10(-4) CM2/(V.S) (RSD = 3.9%; n = 3), a decrease of only 8% below that of the initially measured value. Separations performed on these devices generated 80 000-100 000 theoretical plates in 6- 14 s for both tetramethylrhodamine succidimidyl ester and fluorescein-5-isothiocyanate derivatized amino acids. The separation distance was 3.5 cm. Plots of peak variance vs analyte migration times gave diffusion coefficients which indicate that the separation efficiencies are within 15% of the diffusion limit.
引用
收藏
页码:1414 / 1422
页数:9
相关论文
共 80 条
[21]   A microfabricated fluorescence-activated cell sorter [J].
Fu, AY ;
Spence, C ;
Scherer, A ;
Arnold, FH ;
Quake, SR .
NATURE BIOTECHNOLOGY, 1999, 17 (11) :1109-1111
[22]   An integrated microfabricated cell sorter [J].
Fu, AY ;
Chou, HP ;
Spence, C ;
Arnold, FH ;
Quake, SR .
ANALYTICAL CHEMISTRY, 2002, 74 (11) :2451-2457
[23]   Microfluidic memory and control devices [J].
Groisman, A ;
Enzelberger, M ;
Quake, SR .
SCIENCE, 2003, 300 (5621) :955-958
[24]  
Harrison DJ, 2003, LAB-ON-A CHIP: MINIATURIZED SYSTEMS FOR ( BIO ) CHEMICAL ANALYSIS AND SYNTHESIS, P249, DOI 10.1016/B978-044451100-3/50013-9
[25]  
Haugland R.P., 1996, Handbook of Fluorescent Probes and Research Chemicals
[26]   Hydrophobicity recovery of polydimethylsiloxane after exposure to corona discharges [J].
Hillborg, H ;
Gedde, UW .
POLYMER, 1998, 39 (10) :1991-1998
[27]   Tailoring the surface properties of poly(dimethylsiloxane) microfluidic devices [J].
Hu, SW ;
Ren, XQ ;
Bachman, M ;
Sims, CE ;
Li, GP ;
Allbritton, NL .
LANGMUIR, 2004, 20 (13) :5569-5574
[28]   Surface-directed, graft polymerization within microfluidic channels [J].
Hu, SW ;
Ren, XQ ;
Bachman, M ;
Sims, CE ;
Li, GP ;
Allbritton, NL .
ANALYTICAL CHEMISTRY, 2004, 76 (07) :1865-1870
[29]   Cross-linked coatings for electrophoretic separations in poly(dimethylsiloxane) microchannels [J].
Hu, SW ;
Ren, XQ ;
Bachman, M ;
Sims, CE ;
Li, GP ;
Allbritton, N .
ELECTROPHORESIS, 2003, 24 (21) :3679-3688
[30]   Surface modification of poly(dimethylsiloxane) microfluidic devices by ultraviolet polymer grafting [J].
Hu, SW ;
Ren, XQ ;
Bachman, M ;
Sims, CE ;
Li, GP ;
Allbritton, N .
ANALYTICAL CHEMISTRY, 2002, 74 (16) :4117-4123