Development of conductive transparent indium tin oxide (ITO) thin films deposited by direct current (DC) magnetron sputtering for photon-STM applications

被引:46
作者
Deng, W [1 ]
Ohgi, T [1 ]
Nejo, H [1 ]
Fujita, D [1 ]
机构
[1] Natl Res Inst Met, Tsukuba, Ibaraki 3050047, Japan
来源
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING | 2001年 / 72卷 / 05期
关键词
D O I
10.1007/s003390100740
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Highly conductive and transparent indium tin oxide (ITO) thin films, each with a thickness of 100 nm, were deposited on glass and Si(100) by direct current (DC) magnetron sputtering under an argon (Ar) atmosphere using an ITO target composed of 95% indium oxide and 5% tin oxide for photon-STM use. X-ray diffraction, STM observations, resistivity and transmission measurements were carried out to study the formation of the films at substrate temperatures between 40 and 400 degreesC and the effects of thermal annealing in air between 200 and 400 degreesC for between 1 and 5 h. The film properties were highly dependent on deposition conditions and on post-deposition film treatment. The films deposited under an Ar atmosphere pressure of similar to 1.7 x 10(-3) Torr by DC power sputtering (100 W) at substrate temperatures between 40 and 400 degreesC exhibited resistivities in the range 3.0-5.7 x 10(-5) Ohm m and transmissions in the range 71%-79%. After deposition and annealing in air at 300 degreesC for Ih, the films showed resistivities in the range 2.9-4.0 x 10(-5) Ohm m and transmissions in the range 78%-81%. Resistivity and transmission measurements showed that in order to improve conductive and transparent properties, 2 h annealing in air at 300 degreesC was necessary. X-ray diffraction data supported the experimental measurements of resistivity and transmission on the studies of annealing time. The surface roughness and film uniformity improve with increasing substrate temperature. STM observations found the ITO films deposited at a substrate temperature of 325 degreesC, and up to 400 degreesC, had domains with crystalline structures. After deposition and annealing in air at 300 degreesC for 1 h the films still exhibited similar domains. However, after deposition at substrate temperatures from 40 degreesC to 300 degreesC, and annealing in air at 300 degreesC for 1 h, the films were shown to be amorphous. More importantly, the STM studies found that the ITO film surfaces were most likely to break after deposition at a substrate temperature of 325 degreesC and annealing in air at 300 degreesC for 2 or 3 h. Such findings give some inspiration to us in interpreting the effects of annealing on the improvement of conductive and transparent properties and on the transition of phases. In addition, correlations between the conductive/transparent properties and the phase transition, the annealing time and the phase transition, and the conductive/transparent properties and the annealing time have been investigated.
引用
收藏
页码:595 / 601
页数:7
相关论文
共 24 条
[11]   Improved operational stability of polyfluorene-based organic light-emitting diodes with plasma-treated indium-tin-oxide anodes [J].
Kim, JS ;
Friend, RH ;
Cacialli, F .
APPLIED PHYSICS LETTERS, 1999, 74 (21) :3084-3086
[12]   Indium-tin oxide treatments for single- and double-layer polymeric light-emitting diodes: The relation between the anode physical, chemical, and morphological properties and the device performance [J].
Kim, JS ;
Granstrom, M ;
Friend, RH ;
Johansson, N ;
Salaneck, WR ;
Daik, R ;
Feast, WJ ;
Cacialli, F .
JOURNAL OF APPLIED PHYSICS, 1998, 84 (12) :6859-6870
[13]  
Lan JH, 1997, MATER RES SOC SYMP P, V424, P347
[14]   HIGH CONDUCTING LARGE AREA INDIUM TIN OXIDE ELECTRODES FOR DISPLAYS PREPARED BY DC MAGNETRON SPUTTERING [J].
LATZ, R ;
MICHAEL, K ;
SCHERER, M .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 1991, 30 (2A) :L149-L151
[15]  
MARUYAMA E, 1995, SOLID STATE PHENOM, V44, P863
[16]   INDIUM TIN OXIDE THIN-FILMS PREPARED BY CHEMICAL VAPOR-DEPOSITION [J].
MARUYAMA, T ;
FUKUI, K .
THIN SOLID FILMS, 1991, 203 (02) :297-302
[17]   Crystal growth of ITO films prepared by DC magnetron sputtering on C film [J].
Morikawa, H ;
Sumi, H ;
Kohyama, M .
THIN SOLID FILMS, 1996, 281 :202-205
[18]   Two-dimensional spatial profiles of plasma parameters in DC reactive magnetron sputtering of indium-tin-oxide [J].
Muta, M ;
Ohgushi, S ;
Matsuda, Y ;
Fujiyama, H .
THIN SOLID FILMS, 1999, 341 (1-2) :221-224
[19]   Amorphous silicon photodiode thin film transistor image sensor with diode on top structure [J].
Powell, MJ ;
Glasse, C ;
French, ID ;
Franklin, AR ;
Hughes, JR ;
Curran, JE .
AMORPHOUS AND MICROCRYSTALLINE SILICON TECHNOLOGY - 1997, 1997, 467 :863-868
[20]   Low resistivity indium tin oxide films deposited by unbalanced DC magnetron sputtering [J].
Shin, SH ;
Shin, JH ;
Park, KJ ;
Ishida, T ;
Tabata, O ;
Kim, HH .
THIN SOLID FILMS, 1999, 341 (1-2) :225-229