A NEW OXIDATION-RESISTANT COSI2 PROCESS FOR SELF-ALIGNED SILICIDATION (SALICIDE) TECHNOLOGY

被引:2
作者
LOU, YS [1 ]
WU, CY [1 ]
CHENG, HC [1 ]
机构
[1] NATL CHIAO TUNG UNIV,INST ELECTR,HSINCHU,TAIWAN
关键词
D O I
10.1016/0038-1101(93)90071-W
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
This paper presents a new oxidation-resistant and self-aligned CoSi2 process using amorphous-Si (a-Si)/Co bilayer metallization. It is shown that, even in an environment without introducing any flowing inert gas, the detrimental reaction between Co metal and ambient impurities, e.g. O2 and H2O, can be completely impeded by a covered thin a-Si layer during the thermal silicidation cycle. Moreover, despite a capped a-Si layer over Co film, the satisfactory self-aligned silicidation properties can be retained if the initial silicidation temperature is kept below 500-degrees-C in N2 ambient. Furthermore, the dependences of both oxidation-resistant and self-aligned silicidation properties on the thicknesses of a-Si and Co films are studied in detail. Based on experimental analysis, the allowed process window for the a-Si film thickness can be determined and is shown to increase with increasing the Co film thickness. An empirical process rule is experimentally obtained to determine the optimal thickness relation between a-Si and Co films for the a-Si/Co bilayer process. Thus, a simple and practical self-aligned CoSi2 process with extremely high immunity to ambient impurities is proposed for SALICIDE applications.
引用
收藏
页码:75 / 83
页数:9
相关论文
共 18 条
[1]   DEVELOPMENT OF THE SELF-ALIGNED TITANIUM SILICIDE PROCESS FOR VLSI APPLICATIONS [J].
ALPERIN, ME ;
HOLLAWAY, TC ;
HAKEN, RA ;
GOSMEYER, CD ;
KARNAUGH, RV ;
PARMANTIE, WD .
IEEE TRANSACTIONS ON ELECTRON DEVICES, 1985, 32 (02) :141-149
[2]   FORMATION OF THIN-FILMS OF COSI2 - NUCLEATION AND DIFFUSION MECHANISMS [J].
DHEURLE, FM ;
PETERSSON, CS .
THIN SOLID FILMS, 1985, 128 (3-4) :283-297
[3]   APPLICATION OF THE SELF-ALIGNED TITANIUM SILICIDE PROCESS TO VERY LARGE-SCALE INTEGRATED N-METAL-OXIDE-SEMICONDUCTOR AND COMPLEMENTARY METAL-OXIDE-SEMICONDUCTOR TECHNOLOGIES [J].
HAKEN, RA .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1985, 3 (06) :1657-1663
[4]   SOLID-II - HIGH-VOLTAGE HIGH-GAIN KILO-ANGSTROM-CHANNEL-LENGTH CMOSFETS USING SILICIDE WITH SELF-ALIGNED ULTRASHALLOW (3S) JUNCTION [J].
HORIUCHI, M ;
YAMAGUCHI, K .
IEEE TRANSACTIONS ON ELECTRON DEVICES, 1986, 33 (02) :260-269
[5]   SIMULTANEOUS FORMATION OF SILICIDE OHMIC CONTACTS AND SHALLOW P+-N JUNCTIONS BY ION-BEAM MIXING AND RAPID THERMAL ANNEALING [J].
KWONG, DL ;
MEYERS, DC ;
ALVI, NS .
IEEE ELECTRON DEVICE LETTERS, 1985, 6 (05) :244-246
[6]   THE PROCESS WINDOW OF A-SI/TI BILAYER METALLIZATION FOR AN OXIDATION-RESISTANT AND SELF-ALIGNED TISI2 PROCESS [J].
LOU, YS ;
WU, CY ;
CHENG, HC .
IEEE TRANSACTIONS ON ELECTRON DEVICES, 1992, 39 (08) :1835-1843
[7]   SELF-ALIGNED SILICIDES OR METALS FOR VERY LARGE-SCALE INTEGRATED-CIRCUIT APPLICATIONS [J].
MURARKA, SP .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1986, 4 (06) :1325-1331
[8]   SELF-ALIGNED COBALT DISILICIDE FOR GATE AND INTERCONNECTION AND CONTACTS TO SHALLOW JUNCTIONS [J].
MURARKA, SP ;
FRASER, DB ;
SINHA, AK ;
LEVINSTEIN, HJ ;
LLOYD, EJ ;
LIU, R ;
WILLIAMS, DS ;
HILLENIUS, SJ .
IEEE TRANSACTIONS ON ELECTRON DEVICES, 1987, 34 (10) :2108-2115
[9]   REFRACTORY SILICIDES FOR INTEGRATED-CIRCUITS [J].
MURARKA, SP .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1980, 17 (04) :775-792
[10]  
MURARKA SP, 1983, SILICIDES VLSI APPLI